Rayleigh waves

I want to establish a system that can measure grain size by rayleigh waves.
Is there anybody that help me, how can I measure grain size by this way and
how can establish that experiment setup.
thanks for your helps.


 
 Reply 
 
Ernst Niederleithinger
R & D, -
BAM (Fed. inst. for material research and testing, Germany, Joined Jun 2001, 7

Ernst Niederleithinger

R & D, -
BAM (Fed. inst. for material research and testing,
Germany,
Joined Jun 2001
7
01:00 Sep-11-2001
Re: Rayleigh waves
: I want to establish a system that can measure grain size by rayleigh waves.
: Is there anybody that help me, how can I measure grain size by this way and
: how can establish that experiment setup.
: thanks for your helps.

Very interesting. Rayleigh waves are very popular in geophysical/geotechnical testing
(SASW method).
Grain size: R. Chammas (of French streets and bridges authority)
has done FE modelling on the influence of inclusions
on surface waves (rabih.chammas@lcps.fr).
Please keep me informed!





 
 Reply 
 
Bruce Maxfield
Engineering, electronics and instrumentation
Analogic Engineering, Inc., USA, Joined Jan 2000, 10

Bruce Maxfield

Engineering, electronics and instrumentation
Analogic Engineering, Inc.,
USA,
Joined Jan 2000
10
01:24 Sep-12-2001
Re: Rayleigh waves
: I want to establish a system that can measure grain size by rayleigh waves.
: Is there anybody that help me, how can I measure grain size by this way and
: how can establish that experiment setup.
: thanks for your helps.
.

I have been working with Fallon Ultrasonics, Inc. on methods to deduce residual stresses from elastic wave velocity measurements. As part of this work, I have used Rayleigh wave ( relatively insensitive to stress) and critically refracted longitudinal wave (much more sensitive to stress) velocities (actually, travel times). These waves have been generated using focused ultrasonic beams like those generated by spherically and cylindrically focused ultrasonic transducers, by plastic wedges of an appropriate angle and by plane waves at an angle to the specimen surface in a water bath. Each of these methods has one or more advantages over the others. In all cases of practical alloys that we have studied, grain scattering is the material parameter that limits the highest frequency that can be used. We have not yet done much quantitative work with respect to determining grain size but it is very clear that the attenuation of these waves is strongly influenced by grain scattering at higher frequencies (as expected) and that this attenuation can be measured with relative ease. There are several corrections that must be made to the measured attenuation in order to obtain the grain scattering term which can be used to deduce the "mean" grain diameter in the region of material being sampled by the elastic wave. If you care to let me know the material and grain size range that is of interest to you, I can give you some general idea of the magnitude of effort that will be required.


 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window