02:59 Sep-25-2001
accoustic emmision application articles

I am studing on A.E. application as my B.s final project.please help me to find cool link about this subject.


 
 Reply 
 
Jens Forker
Jens Forker
04:19 Sep-25-2001
Re: accoustic emmision application articles
Hi,

welcome to visit www.vallen.de (we are specialized on acoustic emission). If you would like further information, please let me know.

Regards
Jens Forker
Vallen-Systeme GmbH

: I am studing on A.E. application as my B.s final project.please help me to find cool link about this subject.
.



 
 Reply 
 
Dr.Sotirios J. Vahaviolos
R & D, -
MISTRAS Group, Inc., USA, Joined Jan 2000, 15

Dr.Sotirios J. Vahaviolos

R & D, -
MISTRAS Group, Inc.,
USA,
Joined Jan 2000
15
05:19 Sep-25-2001
Re: accoustic emmision application articles
: I am studing on A.E. application as my B.s final project.please help me to find cool link about this subject.
.
There exists a large volume of literature around the world.The best sources for AE reading are :
.ASNT(American Society of NDT)Acoustic Emission Handbook Edited by our Dr. Ron Miller and Paul
McIntire of ASNT
.Progress in Acoustic Emission Proceedings from the Japanese AE Symposia(several volumes)
.Several ASTM(American Society of Testing and Materials)Books starting with STP-505 to the latest one STP-1353
.The Journal of Acoustic Emission Edited by Prof. K.Ono of UCLA
I hope this gives you a good start.Besides commercial companies in AE can provide you with additional Applications
Reports available upon request from any of our Subsidiaries Worldwide.Also our Company MISTRAS Holdings Group
provides scholarships and cooperates with several Professors in supporting students in AE.
Good luck to you
Sotirios J. Vahaviolos


 
 Reply 
 
Jijo Chakkappan
Jijo Chakkappan
01:56 Aug-29-2002
Re: accoustic emmision application articles
We are looking for a company who can do accoustic emmision testing for the 14 nos. of floating roof steel storage tanks. Could u please advise us name & contacas of some companies


 
 Reply 
 
Phil Thayer
Phil Thayer
06:46 Aug-29-2002
Re: accoustic emmision application articles
: We are looking for a company who can do accoustic emmision testing for the 14 nos. of floating roof steel storage tanks. Could u please advise us name & contacas of some companies
.
You should contact QSL-Plus 610-497-0400. They have been in AE test business for over 25 years and have tested thousands of tanks Worldwide. They have developed proven TANKPAC test procedure. Oh, web page pacndt.com.


 
 Reply 
 

Product Spotlight

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window