UT gauges

I have a need for a UT gauge that can do the following:

Display on the UT gauge screen the isometric drawing of the pipeline or vessel that is been tested.

Indicate on the isometric drawing spots that have depleted beyond a set value (wall thickness).

Download both readings and drawing onto a computer.

The UT gauge should be able to store a minimum of 20,000 data.

Please any assistance will be highly appreciated.



    
 
 Reply 
 
Marius Iulian DINU
NDT Inspector, Pre-service and In-Service Inspections
General Electric - Life Extension Services, Romania, Joined Oct 1999, 5

Marius Iulian DINU

NDT Inspector, Pre-service and In-Service Inspections
General Electric - Life Extension Services,
Romania,
Joined Oct 1999
5
09:13 Oct-11-2001
Re: UT gauges
On my knowledge, there is no UT gauge available on market that can do what you want (isometric drawings on UT gauge).

However, you can use any UT gauge that have a datalogger, and then transfer the thickness data in a computer that has installed a specialized Erosion / Corrosion software - for example UltraPIPE from Krautkramer. This software can do all you want - including interface with AutoCAD for viewing and editing the isometric drawings. It can also upload site data (thickness monitoring location) for the UT operator.

If you want to know more about this software go to www.ultrapipe.com

Marius

: I have a need for a UT gauge that can do the following:
.
: Display on the UT gauge screen the isometric drawing of the pipeline or vessel that is been tested.
.
: Indicate on the isometric drawing spots that have depleted beyond a set value (wall thickness).
.
: Download both readings and drawing onto a computer.
.
: The UT gauge should be able to store a minimum of 20,000 data.
.
: Please any assistance will be highly appreciated.
.



    
 
 Reply 
 
Art Leach
Sales
GE Inspection Technologies, USA, Joined Apr 2001, 12

Art Leach

Sales
GE Inspection Technologies,
USA,
Joined Apr 2001
12
05:25 Oct-12-2001
Re: UT gauges
Willy,

You should really look at the Krautkramer DMS 2 use with the UltraPIPE software program. All equipment TML's are set-up in UltraPIPE, sent to the DMS 2 allowing the inspector to take the readings then send the readings back to the program. The new data is used to re-calculate corrosion rates, inspection and retirement dates for the equipment.

Old readings from the previous survey can be uploaded for an on the fly evaluation of old vs. current readings. A-Scans, B-Scans and MicroGRID attachments can also be stored and analyzed in UltraPIPE.

Contact your local Krautkramer sales representative for a demonstration of the DMS 2 and visit the UltraPIPE web site at www.ultrapipe.com for information on the software.


The idea of dislaying the isographic on the screen is a good idea, but the displays used in thickness gauges, even though they are high resolution for the gauge, still are not adaquate for displaying iso drawings, markers and text.

Art Leach.


: I have a need for a UT gaugethat can do the following:
.
: Display on the UT gauge screen the isometric drawing of the pipeline or vessel that is been tested.
.
: Indicate on the isometric drawing spots that have depleted beyond a set value (wall thickness).
.
: Download both readings and drawing onto a computer.
.
: The UT gauge should be able to store a minimum of 20,000 data.
.
: Please any assistance will be highly appreciated.
.



    
 
 Reply 
 
Meindert Anderson
Director
Olympus, USA, Joined Dec 1999, 5

Meindert Anderson

Director
Olympus,
USA,
Joined Dec 1999
5
06:28 Oct-12-2001
Re: UT gauges
Mr. MacChiourlu

There are many other very good corrosion thickness gages (with A-Scan display)on the market that are compatible with UltraPipe software. Some of these gages may have measurement features that the unit described below does not offer ... and I hope you will find the time to check out these other gages.

One of the rules for this wonderful Forum is: "Do not post advertisements for commercial products". It is unfortunate that some members do not adhere to this rule.

Best regards,
Meindert Anderson
Panametrics, Inc.


Willy,
.
: You should really look at the Krautkramer DMS 2 use with the UltraPIPE software program. All equipment TML's are set-up in UltraPIPE, sent to the DMS 2 allowing the inspector to take the readings then send the readings back to the program. The new data is used to re-calculate corrosion rates, inspection and retirement dates for the equipment.
.
: Old readings from the previous survey can be uploaded for an on the fly evaluation of old vs. current readings. A-Scans, B-Scans and MicroGRID attachments can also be stored and analyzed in UltraPIPE.
.
: Contact your local Krautkramer sales representative for a demonstration of the DMS 2 and visit the UltraPIPE web site at www.ultrapipe.com for information on the software.
.
:
: The idea of dislaying the isographic on the screen is a good idea, but the displays used in thickness gauges, even though they are high resolution for the gauge, still are not adaquate for displaying iso drawings, markers and text.
.
: Art Leach.
.
.
:
: : I have a need for a UT gauge that can do the following:
: .
: : Display on the UT gauge screen the isometric drawing of the pipeline or vessel that is been tested.
: .
: : Indicate on the isometric drawing spots that have depleted beyond a set value (wall thickness).
: .
: : Download both readings and drawing onto a computer.
: .
: : The UT gauge should be able to store a minimum of 20,000 data.
: .
: : Please any assistance will be highly appreciated.
: .
.



    
 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

SONOAIR - air-coupled Phased Array Ultrasonic Inspection System

For highly attenuating materials, the performance of the system is critical. The ultrasonic sensors,
...
the scanning area and the system settings should be flexibly adapted to the test task and the material. These high expectations are met with the new and modular testing system SONOAIR. With the world’s first air-coupled phased-array UT inspection system SONOAIR we developed a technology that works with up to 4 transmitter and receiver channels with freely configurable square wave burst transmitters as wells as low noise receiving amplifiers.
>

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window