where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

WesDyne International (AMDATA Products)
WesDyne is an engineering and technical services firm dedicated to providing standard and custom nondestructive examinations (NDE) products and systems
3256 views
Technical Discussions
Stan
NDT Inspector,
Canada, Joined Jan 2009, 31

Stan

NDT Inspector,
Canada,
Joined Jan 2009
31
21:27 Oct-20-2010
Sound Beam Focal Region

Hi:
Does any one know of a formula to measure or approximate the length of the focal region of a sound beam.
Stan

 
 Reply 
 
Gerhard Splitt
R & D, -
Private, Germany, Joined Nov 1998, 38

Gerhard Splitt

R & D, -
Private,
Germany,
Joined Nov 1998
38
21:47 Oct-20-2010
Re: Sound Beam Focal Region
In Reply to Stan at 21:27 Oct-20-2010 (Opening).

Hi Stan,
as a rule of thumb, the focus range (-6 dB) is roughly 1/3 in front of the focus and 2/3 behind the focus. For an exact calculation see the web site of imasonic: http://imasonic.com/Industry/IM_Design.php.

Gerhard

 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
22:30 Oct-20-2010
Re: Sound Beam Focal Region
In Reply to Stan at 21:27 Oct-20-2010 (Opening).

You may also find useful the beam equations on page 43 of the Panametrics-NDT transducer catalog, which you can download through the link below.

http://www.olympus-ims.com/panametrics-ndt-ultrasonic/pdf/

 
 Reply 
 
Carlos Correia
R & D, - -
UCV & EGROUP, Venezuela, Joined Oct 2008, 120

Carlos Correia

R & D, - -
UCV & EGROUP,
Venezuela,
Joined Oct 2008
120
03:29 Oct-21-2010
Re: Sound Beam Focal Region
In Reply to Tom Nelligan at 22:30 Oct-20-2010 .

Hello Stan, the following equation was extracted from AUTOMATIC ULTRASONIC TESTING FOR PIPELINE GIRTH WELDS (chapter 2) an excellent book from our friend Ed Ginzel.
d=0.2568xDxSf
Where
Sf=F/N
F: Focal length
N: Near field
D: transducer diameter
Sf: Normalized focal length
d: beam diameter at -6dB

 
 Reply 
 
Gerhard Splitt
R & D, -
Private, Germany, Joined Nov 1998, 38

Gerhard Splitt

R & D, -
Private,
Germany,
Joined Nov 1998
38
09:23 Oct-21-2010
Re: Sound Beam Focal Region
In Reply to Stan at 21:27 Oct-20-2010 (Opening).

Hi Carlos,
your formula calculates the beam diameter (beam width) at the focus point; not the length of the focal region, which Stan has asked for.

Gerhard

 
 Reply 
 
Stan
NDT Inspector,
Canada, Joined Jan 2009, 31

Stan

NDT Inspector,
Canada,
Joined Jan 2009
31
01:45 Oct-22-2010
Re: Sound Beam Focal Region
In Reply to Gerhard Splitt at 09:23 Oct-21-2010 .

Gerhard:
If my understanding is correct, then for a flat unfocused transducer, where Sf = F/N, Focal Length and Near Field Length should be equal and therefore Sf should equal 1. Is this correct?

Stan

 
 Reply 
 
Gerhard Splitt
R & D, -
Private, Germany, Joined Nov 1998, 38

Gerhard Splitt

R & D, -
Private,
Germany,
Joined Nov 1998
38
09:33 Oct-22-2010
Re: Sound Beam Focal Region
In Reply to Stan at 01:45 Oct-22-2010 .

Stan,
that's right!
For N we have as a good approximation the well known formula:
N=D²*f/(4v)
with D= transducer diameter
f=frequency
v= sound velocity in the material under test, e.g. steel.

Regards,
Gerhard

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1285

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1285
14:29 Oct-27-2010
Re: Sound Beam Focal Region
In Reply to Stan at 21:27 Oct-20-2010 (Opening).

Stan, it sounds like you are looking to calculate the depth of field for the 6dB working range of the soundpath.
There is a nice application avaialble on the Immasonic website at http://www.imasonic.com/Industry/IM_Design.php
You enter the appropriate values (for a single element round probe) and then press Calculation to see the values filled in. It is interesting to see how the radius of curvature and the focal distance are not the same! Focusing quickly reduces the useful working range (depth of field) of the beam.

 
 Reply 
 
Stan
NDT Inspector,
Canada, Joined Jan 2009, 31

Stan

NDT Inspector,
Canada,
Joined Jan 2009
31
22:22 Oct-29-2010
Re: Sound Beam Focal Region
In Reply to Ed Ginzel at 14:29 Oct-27-2010 .

Thanks Ed:
I played around with this, and I am wondering how the Radius of Curvature is related to the Focal distance programmed into the focal laws for a PA instrument. Are they the same number?
Stan

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1285

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1285
22:40 Oct-31-2010
Re: Sound Beam Focal Region
In Reply to Stan at 21:27 Oct-20-2010 (Opening).

Stan, the ROC (radius of curvature) is not really related in any direct way to the PA focusing in the focal laws. They use the Fermat principle to compute the shortest travel "time" to the desired focal point.
You can now order a curved passive plane on a linear array (helps reduce over-sizing of length in a linear scan). This would use the equation seen on the Imasonic site. It is intersting to see that the optical focal point and the acoustic focal point are not identical! For the focal point defined by the ROC to equal the distance in the test material, the velocity of the test material must be 1m/s. E.g. if the 5MHz 10mm diameter probe had a 50mm ROC the beam would focus at 50mm from the probe only if the material velocity was 1m/s.

 
 Reply 
 

Product Spotlight

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>