Ultrasonic test in HDPE

Hi colleagues of NDT, please, i need information, about ultrasonis test in HDPE"s piping, since some years behind use the ASTM F 600 that already is not used: I have my doubts with regard to the use of the UT with the equipments and conventional transducer used for carbon steel.
Thanks


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
02:46 Apr-10-2008
Re: Ultrasonic test in HDPE
In NDT.net you find some articles of this topic:

Insight 2007-02
Ultrasonic phased array inspection of electrofusion joints in polyethylene pipes
D. Caravaca, C. Bird, D. Kleiner
TWI Ltd, Cambridge [United Kingdom]
http://www.ndt.net/article/insight/papers/insi.49.2.83.pdf

ECNDT 2006-09
THE ULTRASONIC PHASED ARRAY INSPECTION OF ELECTROFUSION JOINTS IN POLYETHYLENE PIPES
C. Bird, D. Caravaca, D. Kleiner
TWI Ltd, Cambridge [United Kingdom]
http://www.ndt.net/article/ecndt2006/doc/Mo.2.6.2.pdf

NDT.net 1996-04
UT and X-Ray NDT of Butt Fusion Welds in PE Pipe, Overview
G. Georgiou, I. Munns
TWI Ltd, Cambridge [United Kingdom]
http://www.ndt.net/article/twi/twi.htm

----------- Start Original Message -----------
: Hi colleagues of NDT, please, i need information, about ultrasonis test in HDPE"s piping, since some years behind use the ASTM F 600 that already is not used: I have my doubts with regard to the use of the UT with the equipments and conventional transducer used for carbon steel.
: Thanks
------------ End Original Message ------------




 
 Reply 
 
A.Ahmadi
A.Ahmadi
14:52 Jun-22-2011
Re: Ultrasonic test in HDPE
In Reply to Rolf Diederichs at 02:46 Apr-10-2008 .

Dear sir,
my company need buy 1 unit for test hdpe electro fusion fittings 25-160mm

best regards

 
 Reply 
 
coolguy
coolguy
15:29 Jun-22-2011
Re: Ultrasonic test in HDPE
In Reply to A.Ahmadi at 14:52 Jun-22-2011 .

Hello Buddy,

You may contact Olympus NDT as they have already conducted some R7D of these tests.

Please find the link below

http://www.olympus-ims.com/en/applications/ultrasonic-tofd-butt-fusion/

You can contact carl.mercier@olympusndt.com

 
 Reply 
 
Christoph Schnitger
Christoph Schnitger
19:22 Jun-22-2011
Re: Ultrasonic test in HDPE
In Reply to A.Ahmadi at 14:52 Jun-22-2011 .

Dear Sirs,

since 2004 we are offering this kind of UT equipment here on the german market. We used a special kind of phased array system; - it is also a question to have the right probe !

We have this system on stock for different HDPE piping, different wall thicknesses and also
adapters for different fitting styles.

 
 Reply 
 
Raul Leon
Raul Leon
01:59 Nov-02-2011
Re: Ultrasonic test in HDPE
In Reply to vicente domingo encina at 01:06 Apr-07-2008 (Opening).

We have been using TOFD and Phased Array techniques to test joints in HDPE since 2004 in the mining and petrochemical markets. We had, so far, no failures on joints inspected with this methodology and using acceptance and reject criteria developed by large engineering corporations which we have worked in the past. These techniques are getting better with time, and we believe that the codes will include some of these techniques in the future.

 
 Reply 
 
Meh Iskandar
Meh Iskandar
20:50 Nov-06-2011
Re: Ultrasonic test in HDPE
In Reply to vicente domingo encina at 01:06 Apr-07-2008 (Opening).

Hi Encina,

There is a company named "KNDT" that offers some products for your work. It has the worth to see this too.
http://www.kndt.co.kr/us/aim33.htm

It seems that the lack of worldwide accepted code is the main problem in using PA UT in the application of HDPE's inspection.

Good luck

 
 Reply 
 

Product Spotlight

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window