00:16 Jan-15-2002
Look for under ground pipeline corrosion inspection system

Dear all:
I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!


 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:46 Jan-15-2002
Re: Look for under ground pipeline corrosion inspection system
You can contact No Pig at Email fino@finoag.com

Mark your email for the attention of Michael Broderick.

Their tel number is +49 5063 9599

WE have been looking at No Pig a lot plus other underground inspection techniques. If you need assistance please feel free to contact me direct.


 
 Reply 
 
Brant Shields
Brant Shields
08:16 Feb-20-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!
.

Have you considered Guided Ultrasonics for your underground piping? Contact us for any information or questions you may have.


 
 Reply 
 
Peter
Consultant
PQS, United Kingdom, Joined Jan 2002, 7

Peter

Consultant
PQS,
United Kingdom,
Joined Jan 2002
7
08:11 Feb-21-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!

Guided Ultrasonics Ltd manufacture Wavemaker SE16 guided wave pipe screening system which is in use worldwide. Look at website www.guided-ultrasonics.com or contact Peter@guided-ultrasonics.com for more info.



 
 Reply 
 
Jim Yukes
Jim Yukes
09:29 Feb-22-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!
.
Can you give more information about the pipe to be inspected? We can supply an electromagnetic system for small diameter pipes and may be able to do something for larger diameters depending on the length of the line. Do you have access to the pipe OD? E-Pit will inspect from the OD through coatings. See : www.russelltech.com


 
 Reply 
 
Jim Yukes
Jim Yukes
09:29 Feb-22-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!
.
Can you give more information about the pipe to be inspected? We can supply an electromagnetic system for small diameter pipes and may be able to do something for larger diameters depending on the length of the line. Do you have access to the pipe OD? E-Pit will inspect from the OD through coatings. See : www.russelltech.com


 
 Reply 
 
Jamie Gauthier
Jamie Gauthier
00:45 Feb-22-2002
Re: Look for under ground pipeline corrosion inspection system
We have a system that can determine underground corrosion. Please call RTD Quality Services Inc. for further details.

Toll Free: 800-661-0066
Reception: 780-440-6600
Fax: 780-440-2538
Web: www.rtdquality.com
Email: jgauthier@rtdquality.com


 
 Reply 
 
David
David
06:09 Feb-25-2002
Re: Look for under ground pipeline corrosion inspection system
We are from a third party inspection company having international operation. We provide one-stop NDT solutions for the oil and gas pipeline inspections.

We are able to inspect for underground pipeline inspection without the need to remove insulation (dig)or pigging up to 100 metres depending on the anticipated condition of the pipe. Only one spot for each measurement is required at exposed areas like road crossing etc. The equipment we are using is sophisticated and reliable.

Other services available include corrosion under insulation (CUI) inspection where the need to remove insulation (up to 150 mm) is eliminated.

Kindly furnish us with more info on the pipeline i.e. ID, OD, length, base material, drawings (if necessary) for us to evaluate the situation and provide you the appropriate solution for your attention.

Rgds, David.


 
 Reply 
 
Musarrat Imam
Musarrat Imam
03:18 Jul-02-2002
Re: Look for under ground pipeline corrosion inspection system
We have a pipe sea water under ground carbonsteel pipe 72 and 84" dia. The pipe is corroded externally. The pipe is protected inside by glassflaking and externally hot applied bitumen membrane. we want to refurbish the pipe externally online inorder to withstand the pipe 10-15 years. The pipe was laid in 1970. please advise
1. do you have any technology which can find out the corrosion precentage of the pipe.
2. What kind of coating you will prefer to protect the pipe.

regards,
M.imam
mimam@qafco.com.qa


 
 Reply 
 
Bhaskar
Bhaskar
11:44 Dec-14-2010
Re: Look for under ground pipeline corrosion inspection system
In Reply to David at 06:09 Feb-25-2002 .

We would like to know the system for wall thickness measurement of underground pipeline without exposure to outside (ie burried pipeline of 1 to 2 KM) Dia ranges from small to Big.

 
 Reply 
 

Product Spotlight

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

On-Demand Webinar: Advanced Ultrasonic Techniques for HTHA Detection & Assessment

In the Oil and Gas industry, High Temperature Hydrogen Attack (HTHA) can occur in steels operating a
...
t high temperature, usually above 205°C (400°F). Early stages of HTHA are very difficult to detect. Join us for a webinar presented by Guy Maes, Zetec Sales Engineer Director. The webinar will demonstrate how advanced ultrasonic techniques are deployed for efficient and reliable HTHA inspections.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>