Ultrasonic test in HDPE

Hi colleagues of NDT, please, i need information, about ultrasonis test in HDPE"s piping, since some years behind use the ASTM F 600 that already is not used: I have my doubts with regard to the use of the UT with the equipments and conventional transducer used for carbon steel.
Thanks


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
02:46 Apr-10-2008
Re: Ultrasonic test in HDPE
In NDT.net you find some articles of this topic:

Insight 2007-02
Ultrasonic phased array inspection of electrofusion joints in polyethylene pipes
D. Caravaca, C. Bird, D. Kleiner
TWI Ltd, Cambridge [United Kingdom]
http://www.ndt.net/article/insight/papers/insi.49.2.83.pdf

ECNDT 2006-09
THE ULTRASONIC PHASED ARRAY INSPECTION OF ELECTROFUSION JOINTS IN POLYETHYLENE PIPES
C. Bird, D. Caravaca, D. Kleiner
TWI Ltd, Cambridge [United Kingdom]
http://www.ndt.net/article/ecndt2006/doc/Mo.2.6.2.pdf

NDT.net 1996-04
UT and X-Ray NDT of Butt Fusion Welds in PE Pipe, Overview
G. Georgiou, I. Munns
TWI Ltd, Cambridge [United Kingdom]
http://www.ndt.net/article/twi/twi.htm

----------- Start Original Message -----------
: Hi colleagues of NDT, please, i need information, about ultrasonis test in HDPE"s piping, since some years behind use the ASTM F 600 that already is not used: I have my doubts with regard to the use of the UT with the equipments and conventional transducer used for carbon steel.
: Thanks
------------ End Original Message ------------




 
 Reply 
 
A.Ahmadi
A.Ahmadi
14:52 Jun-22-2011
Re: Ultrasonic test in HDPE
In Reply to Rolf Diederichs at 02:46 Apr-10-2008 .

Dear sir,
my company need buy 1 unit for test hdpe electro fusion fittings 25-160mm

best regards

 
 Reply 
 
coolguy
coolguy
15:29 Jun-22-2011
Re: Ultrasonic test in HDPE
In Reply to A.Ahmadi at 14:52 Jun-22-2011 .

Hello Buddy,

You may contact Olympus NDT as they have already conducted some R7D of these tests.

Please find the link below

http://www.olympus-ims.com/en/applications/ultrasonic-tofd-butt-fusion/

You can contact carl.mercier@olympusndt.com

 
 Reply 
 
Christoph Schnitger
Christoph Schnitger
19:22 Jun-22-2011
Re: Ultrasonic test in HDPE
In Reply to A.Ahmadi at 14:52 Jun-22-2011 .

Dear Sirs,

since 2004 we are offering this kind of UT equipment here on the german market. We used a special kind of phased array system; - it is also a question to have the right probe !

We have this system on stock for different HDPE piping, different wall thicknesses and also
adapters for different fitting styles.

 
 Reply 
 
Raul Leon
Raul Leon
01:59 Nov-02-2011
Re: Ultrasonic test in HDPE
In Reply to vicente domingo encina at 01:06 Apr-07-2008 (Opening).

We have been using TOFD and Phased Array techniques to test joints in HDPE since 2004 in the mining and petrochemical markets. We had, so far, no failures on joints inspected with this methodology and using acceptance and reject criteria developed by large engineering corporations which we have worked in the past. These techniques are getting better with time, and we believe that the codes will include some of these techniques in the future.

 
 Reply 
 
Meh Iskandar
Meh Iskandar
20:50 Nov-06-2011
Re: Ultrasonic test in HDPE
In Reply to vicente domingo encina at 01:06 Apr-07-2008 (Opening).

Hi Encina,

There is a company named "KNDT" that offers some products for your work. It has the worth to see this too.
http://www.kndt.co.kr/us/aim33.htm

It seems that the lack of worldwide accepted code is the main problem in using PA UT in the application of HDPE's inspection.

Good luck

 
 Reply 
 

Product Spotlight

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window