Hector Guzman
Hector Guzman
04:55 Feb-10-1999
Acoustic Absorption Coefficients

Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

-hector


 
 Reply 
 
Wies³aw Bicz
Wies³aw Bicz
01:14 Feb-10-1999
Re: Acoustic Absorption Coefficients
: Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

: -hector

You can find this information in many books, but it wont help you very much. There are many kinds of plastics on the market, having
different properties. Absorbtion is also very frequency dependent. It is much better to measure it. If you don´t need very high accuracy it is not difficult.
If you need a high accuracy we can help you - we are working on a device doing all such measurements with high accuracy.

W. Bicz


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
05:13 Feb-10-1999
Re: Acoustic Absorption Coefficients



 
 Reply 
 
Grant Gordon
Grant Gordon
06:49 Feb-10-1999
Re: Acoustic Absorption Coefficients
Greetings Hector,
I have recently measured the frequency dependent attenuation values for polycarbonate, acrylic,
linear low density polyethylene, PVC, and a polybutadiene over the frequency range of 1.5 - 9 MHz.
These results are part of a paper to be published in the SPIE Conference proceedings
on Ultrasonic Transducer Engineering to be held in San Diego CA, 20-26 February, 1999. If you are
interested I will send you a hard copy via mail - the electronic file is quite large.
Sincerley
Grant Gordon





 
 Reply 
 
Robert A. Day
Engineering
Milky Way Jewels, USA, Joined Nov 1998, 40

Robert A. Day

Engineering
Milky Way Jewels,
USA,
Joined Nov 1998
40
02:16 Feb-10-1999
Re: Acoustic Absorption Coefficients
: Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

: -hector

I would also recommend Alan Selfridge's paper on measuring ultrasonic properties. His procedure is one of the best procedures for quick reasonably accurate measurements.

I would also warn you that polymers often have different acoustic properties depending on the conditions of manufacture. This includes thicknes as well as temperature and the actual chemistry used. It is essential to keep this in mind when making samples to measure. Thin layers are frequently different than the bulk.


 
 Reply 
 
gina
gina
06:13 Apr-01-2000
Re: Acoustic Absorption Coefficients
: Hi. Does anyone know of a site that will give me a list of materials and their absorption coefficients?

gina


 
 Reply 
 
yuksel guney
yuksel guney
01:42 May-08-2000
Re: Acoustic Absorption Coefficients of polyvinyldenefloride
: : Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for those materials. Specifically I would like to attain the absorption coefficients for polystyrene, polypropylene, and polyethylene.

: : -hector

: You can find this information in many books, but it wont help you very much. There are many kinds of plastics on the market, having
: different properties. Absorbtion is also very frequency dependent. It is much better to measure it. If you don´t need very high accuracy it is not difficult.
: If you need a high accuracy we can help you - we are working on a device doing all such measurements with high accuracy.

: W. Bicz




 
 Reply 
 
paco
paco
07:57 Oct-13-2000
Re: Acoustic Absorption Coefficients
: : Hi. Does anyone know of a good book on 'properties of material' that also contains information such as the acoustic absorption coeffiecinet for materials.


 
 Reply 
 
Ales Globevnik
Ales Globevnik
02:27 Mar-22-2002
Re: Acoustic Absorption Coefficients
Hellooo , I am also looking for absorption coefficients for materials. Please let me know if anybody know where can I found them.



 
 Reply 
 

Product Spotlight

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window