material testing

Members
What standard do you use for checking the elemental composition of stainless steels. What ranges for the different elements. I want to have a document that confirms what PMI or the MTR's give me.


thank you for your reply
Eron

 
 Reply 
 
Hari Kishore
NDT Inspector,
Sievert Group of Companies, India, Joined Nov 2011, 14

Hari Kishore

NDT Inspector,
Sievert Group of Companies,
India,
Joined Nov 2011
14
10:10 Jan-19-2012
Re: material testing
In Reply to eron at 00:29 Jan-19-2012 (Opening).

PMI

 
 Reply 
 
eron
Worldwide, Joined Nov 2011, 5

eron

Worldwide,
Joined Nov 2011
5
01:17 Jan-20-2012
Re: material testing
In Reply to eron at 00:29 Jan-19-2012 (Opening).

I am more looking for the astm or aisi document

 
 Reply 
 
S V Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S V Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
14:52 Jan-20-2012
Re: material testing
In Reply to eron at 01:17 Jan-20-2012 .

There are many standards for elemental analysis. Most of them depend on spectrography, XRF etc. for the main alloying elements and special equipment for Carbon and Sulphur (combustion based methods). Vacuum Emission Spectrometers provide almost a one-stop solution for most of the commercial austenitic stainless steels.

Confirmation of PMI (which is done mostly by Shop floor portable spectroscopy and or XRF) is done using the laboratory VES as mentioned above or wet chemical methods in case of border results.

Regards

Swamy

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window