Urgent!!!

the following data was obtained
1- the peak number inreases with the increase of transducer (probe ) diameter when the other parameter are constant.
2- The band width increases with decrease of transducer (probe) diameter when the other parameters are constant.

please help getting an interpritation for these two results.


 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1286

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1286
00:01 Apr-17-2002
Re: Urgent!!!
Some questions must be answered before this urgent matter can be resolved.
What do you mean by Peak Number.
Is it the number of peaks observed in the near zone?
Is it the peak frequency?
Is it the peak voltage?
Or do you mean centre frequency?
Or something else?

You then state that the bandwidth increases with diameter and claim that all other parameters remain constant.
I SUSPECT the effects of mechanical damping are the main cause of bandwidth variation. But unless you know that the entire construction process of the probe is identical it will be difficult to assert that ALL other parameters are constant.
Perhaps there are parameters varying that you have not considered.
Are these probes contact or immersion evaluated?

Ed

: the following data was obtained
: 1- the peak number inreases with the increase of transducer (probe ) diameter when the other parameter are constant.
: 2- The band width increases with decrease of transducer (probe) diameter when the other parameters are constant.
.
: please help getting an interpritation for these two results.
.



 
 Reply 
 
ISRA
Consultant
isr, Brazil, Joined Apr 2002, 3

ISRA

Consultant
isr,
Brazil,
Joined Apr 2002
3
09:37 May-01-2002
Re: Urgent!!!
I sent this mail 10 days before but i don't know why you don't receive it.

Dear expert
Thanks for giving me of your time to reply my question

by peak number?
i mean the number of half peaks have an amplitude greater than 20% of the
hiegst one (observed by viewing the second backwall echo received from the
V1 block on the oscilloscope)

the kind of probes are broad band normal contact probe (supposed to be
typically constructed)

a third question is
is there any limit for the band width% to judge if it is narrow band or wide
band?





 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1286

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1286
04:10 May-01-2002
Re: Urgent!!!
ISRA:
The number of "peaks" you define is the number of cycles. This varifies my postulation of mechancial variation due to clamping effects on the element.
Smaller dimensioned elements tend to be easier to clamp and thereby limit ring-time. Increased ring-time results in a higher Q-factor [Q=(fc/(f2-f1)] where f2 and f1 are the upper and lower 6dB drop frequencies from the fc or centre frequency.

For a polycrystalline piezo material you will need more damping to reduce the number of cycles over the referenced amplitude for a larger area element as compared to a smaller area element lapped to the same nominal resonant frequency.

As to specific assignments of bandwidth categories; i.e. what percentage bandwidth constitutes broadband or narrowband I do not know what the convention is. I personnally prefer a broadband probe with 1-1.5 cycles and this is usually about a 75-90% bandwidth. But I do not know if a 2 cycled pulse or something less than 70% bandwidth constitutes a narrow band probe.

Band widths greater than 100% are of course possible. But damping rigid crystalline materials to greater and greater amounts eventually kills all useful output. The best option for a useful high bandwidth signal can be had from PVDF and PVTrF materials. These have a very good receiver efficiency (about 7 times more than PZT).

Another potential source of variation is the electrical matching required if there is different capacitance between the electrodes of the large and small probes.
If using a negative spike pulser you can alter the frequency content of the ring by adjusting the pulse duration.

Why are you using the 'second' backwall signal instead of the first? Since you are testing these probes in contact mode you are coupling energy back into the probe's matching plate. Also, because you are testing the frequency content which is, as just discussed above, dependent on the damping of the element you have added another variable in the pressure put on the probe. Now you must consider effects of front loading as well as back loading.

Pages 65-100 of the NDT Handbook Second edition vol 7 by ASNT may be helpful to your design considerations.
Ed

: I sent this mail 10 days before but i don't know why you don't receive it.
.
: Dear expert
: Thanks for giving me of your time to reply my question
.
: by peak number?
: i mean the number of half peaks have an amplitude greater than 20% of the
: hiegst one (observed by viewing the second backwall echo received from the
: V1 block on the oscilloscope)
.
: the kind of probes are broad band normal contact probe (supposed to be
: typically constructed)
.
: a third question is
: is there any limit for the band width% to judge if it is narrow band or wide
: band?
.
.



 
 Reply 
 

Product Spotlight

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window