EAB
EAB
21:41 Aug-09-2011
Computed Radiography and Artifacts
Overall
Style
Insight
Reliability

Great info!

 
 Reply 
 
Tyler
NDT Inspector,
GE Inspection Technologies , USA, Joined May 2011, 24

Tyler

NDT Inspector,
GE Inspection Technologies ,
USA,
Joined May 2011
24
21:54 Aug-09-2011
Re: Computed Radiography and Artifacts
In Reply to EAB at 21:41 Aug-09-2011 (Opening).

zoom image



Another CR artifact pic...this one resulting from a minute scratch that was not easily seen unfiltered or enhanced but with maximum filtering it stands out quit well. If CR systems are set-up to automatically filter (more of a maximum) displayed images, the interpreter may not view this as an artifact!!!
 
 Reply 
 
Justin Byers
Justin Byers
02:11 Dec-07-2011
Re: Computed Radiography and Artifacts
In Reply to Tyler at 21:54 Aug-09-2011 .

Hello Tyler
Do you see many wear marks on your image plates from handling/scanning?
We use CR and have seen indications like the one you highlighted below.
What kind of life are you getting out of the plates?

This is my first time using this site, and am suprised they're aren't more threads dealing with image plate artifacts. This is a major concern here at work as we are at the cusp of moving towards DDA/CR and away from film.

Any info would be great!

Jb

 
 Reply 
 
Tyler
NDT Inspector,
GE Inspection Technologies , USA, Joined May 2011, 24

Tyler

NDT Inspector,
GE Inspection Technologies ,
USA,
Joined May 2011
24
20:55 Jan-13-2012
Re: Computed Radiography and Artifacts
In Reply to Justin Byers at 02:11 Dec-07-2011 .

In regards to your question and concern, we have experienced wear marks on our IP’s but that was with the halo-type portable scanners, any scanner that has direct contact in anyway with the IP’s will reduce the life of the imaging plate. Try to scan the IP's in different locations on the halo types to reduce wear on the rollers of the transport unit.

We have moved away from those type scanners. We have also put a lot of quality controls in place and have been successful in eliminating artifacts observed in the images.

The life dependency on the IP depends on the handling…they can last one to two weeks or last well over 500 exposures, just depends on how careful ALL employees handle them. It seems like every plate manufacturer has a different design in the protective coating. For example one has the best (thickest) protective coating but those results in a loss of resolution. Others have a thinner protective coating which is more prone to damage but the resolution is much better. Just depends on your preference and application.

As long as there is good QC measures put in place your IP’s should last and artifacts should be reduced.

DR is great but I have had clients experience problems in the field with the cables/connections, technicians being to rough on the PC style connections. Manufactures still haven’t addressed these issues so we have had to upgrade on the screws and cables…no big deal though. DR should be wireless in a few more years as the medical industry has a wireless panel available.

I have some suggestions I could send you regarding IP care you if send me your email...the one displayed came back undeliverable.

 
 Reply 
 
David
David
13:18 Jan-16-2012
Re: Computed Radiography and Artifacts
In Reply to Tyler at 20:55 Jan-13-2012 .

Hi All,
I agree with Tyler that DR is sometomes cumbersome due to a cables.
Vidisco ltd has a wireless DR system, it is very much worth looking into.
http://www.vidisco.com/NDTMain.asp

 
 Reply 
 
Tom
NDT Inspector
USA, Joined Jan 2011, 1

Tom

NDT Inspector
USA,
Joined Jan 2011
1
01:10 Jan-17-2012
Re: Computed Radiography and Artifacts
In Reply to David at 13:18 Jan-16-2012 .

What type of plates are you using?

 
 Reply 
 
Tyler
NDT Inspector,
GE Inspection Technologies , USA, Joined May 2011, 24

Tyler

NDT Inspector,
GE Inspection Technologies ,
USA,
Joined May 2011
24
13:08 Feb-29-2012
Re: Computed Radiography and Artifacts
In Reply to Tom at 01:10 Jan-17-2012 .

Mainly GE, but for other contracts we use Fuji and Kodak.

 
 Reply 
 

Product Spotlight

Micro CT

nanoVoxel series has nano-scale resolution by using high voltage X-ray source (from 80-300 kV) wit
...
h micro focal spot and highly sensitive detector including different kinds of big size panel detectors and lens coupling CCD.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window