15:10 Apr-25-2012
how to create artificial flaws in composite plates

I would like to know how to create artificial flaws in composite plates?

Thank you

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
16:54 Apr-25-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

Is this during or after plate manufacture?

 
 Reply 
 
bourgeois yvan
France, Joined Apr 2012, 2

bourgeois yvan

France,
Joined Apr 2012
2
19:03 Apr-25-2012
Re: how to create artificial flaws in composite plates
In Reply to Nigel Armstrong at 16:54 Apr-25-2012 .

It's before plate manufacture.

For example, to create an inclusion, I put a teflon wafer betwenn 2 plies before RTM process.

After creating defects, I would like to control my plates by ultrasonic control.

 
 Reply 
 
flavio vendramin
NDT Inspector,
TAG s.r.l. Cremella ( Lecco ), Italy, Joined Apr 2010, 42

flavio vendramin

NDT Inspector,
TAG s.r.l. Cremella ( Lecco ),
Italy,
Joined Apr 2010
42
10:59 Apr-27-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

After RTM process is possible to create a impact damage at various load or a little spotface by milling.
Before RTM to create delamination by various type of plastic material sheet ( different attenuation during UT inspection) not only PTFE.
bye

 
 Reply 
 
norm woodward
norm woodward
16:00 Apr-27-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

In simulating damage in a composite structure, the first things to ask is what kinds of defects are being sought and what methods of detection am I contemplating.

For example, low frequency eddy current and x-ray might be able to find “disbonds” simulated with flat bottomed holes, yet be useless in finding real disbonds in metallic structures. Likewise, thermography, and again radiography, might be able image Teflon inserts, yet not be as successful in real applications.

Conversely, sometimes the more basic (ruthless) approach is the best approach. A thin, sharp blade shoved into the edge of a glue line of a bonded structure might create the perfect disbond simulation, while a properly applied ball-peen hammer might produce a great “simulation” of in-service impact damage.

 
 Reply 
 

Product Spotlight

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

Echomac® PA Tube Weld Tester

The new robotic Echomac® PA TW is an operator friendly test system for detecting weld zone defects
...
in tube and pipe caused by scarfing or welding processes. Electronic scanning ensures that the entire weld zone is covered without the need for mechanical movement or operator adjustment.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>