how to create artificial flaws in composite plates

I would like to know how to create artificial flaws in composite plates?

Thank you

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
16:54 Apr-25-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

Is this during or after plate manufacture?

 
 Reply 
 
bourgeois yvan
France, Joined Apr 2012, 2

bourgeois yvan

France,
Joined Apr 2012
2
19:03 Apr-25-2012
Re: how to create artificial flaws in composite plates
In Reply to Nigel Armstrong at 16:54 Apr-25-2012 .

It's before plate manufacture.

For example, to create an inclusion, I put a teflon wafer betwenn 2 plies before RTM process.

After creating defects, I would like to control my plates by ultrasonic control.

 
 Reply 
 
flavio vendramin
NDT Inspector,
TAG s.r.l. Cremella ( Lecco ), Italy, Joined Apr 2010, 42

flavio vendramin

NDT Inspector,
TAG s.r.l. Cremella ( Lecco ),
Italy,
Joined Apr 2010
42
10:59 Apr-27-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

After RTM process is possible to create a impact damage at various load or a little spotface by milling.
Before RTM to create delamination by various type of plastic material sheet ( different attenuation during UT inspection) not only PTFE.
bye

 
 Reply 
 
norm woodward
norm woodward
16:00 Apr-27-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

In simulating damage in a composite structure, the first things to ask is what kinds of defects are being sought and what methods of detection am I contemplating.

For example, low frequency eddy current and x-ray might be able to find “disbonds” simulated with flat bottomed holes, yet be useless in finding real disbonds in metallic structures. Likewise, thermography, and again radiography, might be able image Teflon inserts, yet not be as successful in real applications.

Conversely, sometimes the more basic (ruthless) approach is the best approach. A thin, sharp blade shoved into the edge of a glue line of a bonded structure might create the perfect disbond simulation, while a properly applied ball-peen hammer might produce a great “simulation” of in-service impact damage.

 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window