15:10 Apr-25-2012
how to create artificial flaws in composite plates

I would like to know how to create artificial flaws in composite plates?

Thank you

 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
16:54 Apr-25-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

Is this during or after plate manufacture?

 
 Reply 
 
bourgeois yvan
France, Joined Apr 2012, 2

bourgeois yvan

France,
Joined Apr 2012
2
19:03 Apr-25-2012
Re: how to create artificial flaws in composite plates
In Reply to Nigel Armstrong at 16:54 Apr-25-2012 .

It's before plate manufacture.

For example, to create an inclusion, I put a teflon wafer betwenn 2 plies before RTM process.

After creating defects, I would like to control my plates by ultrasonic control.

 
 Reply 
 
flavio vendramin
NDT Inspector,
TAG s.r.l. Cremella ( Lecco ), Italy, Joined Apr 2010, 42

flavio vendramin

NDT Inspector,
TAG s.r.l. Cremella ( Lecco ),
Italy,
Joined Apr 2010
42
10:59 Apr-27-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

After RTM process is possible to create a impact damage at various load or a little spotface by milling.
Before RTM to create delamination by various type of plastic material sheet ( different attenuation during UT inspection) not only PTFE.
bye

 
 Reply 
 
norm woodward
norm woodward
16:00 Apr-27-2012
Re: how to create artificial flaws in composite plates
In Reply to bourgeois yvan at 15:10 Apr-25-2012 (Opening).

In simulating damage in a composite structure, the first things to ask is what kinds of defects are being sought and what methods of detection am I contemplating.

For example, low frequency eddy current and x-ray might be able to find “disbonds” simulated with flat bottomed holes, yet be useless in finding real disbonds in metallic structures. Likewise, thermography, and again radiography, might be able image Teflon inserts, yet not be as successful in real applications.

Conversely, sometimes the more basic (ruthless) approach is the best approach. A thin, sharp blade shoved into the edge of a glue line of a bonded structure might create the perfect disbond simulation, while a properly applied ball-peen hammer might produce a great “simulation” of in-service impact damage.

 
 Reply 
 

Product Spotlight

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

On Demand Webinar: Using Eddy Current Array for Large Areas in Place of Magnetic Particle and Liquid Penetrant Testing

New on-demand webinar on the use of eddy current array (ECA) technology in lieu of liquid penetrant
...
testing (PT) and magnetic particle testing (MT) for large area screenings. The webinar includes an introduction to the technologies with advantages and disadvantages of each. Side by side examples are discussed including aircraft stringers, engine blades, forgings, weld plates & more. View it today.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window