I am looking for people who deal with the testing of polymeric paterials

I am looking for people who deal with the testing of polymeric materials.
I am interesting in investigation polymers and NDT tests of them.
Especially rubbers and composites.
thanks for any help.
aleks.p.k@iaph.bas-net.by





 
 Reply 
 
Richard Kazares
Richard Kazares
09:13 May-29-2002
Re: I am looking for people who deal with the testing of polymeric paterials
Depending on the specifics of your materials and material geometries, our company has recently introduced a low-frequency based UT technology that can be used to inspect multi-layered, internally bonded, thick-section composites and rubber (also rubber-like) materials from a SINGLE SIDE. The system (which we have named TSCOUT - for Thick Section Composite Oblique Ultrasonic Testing) uses either a single set - or an array (up to 4) sensor pairs at specific angles and frequencies designed to optimize UT penetration (and reflection) form normally VERY DIFFICULT to inspect materials - and which (previously) have almost always required dual-sided (through penetration) inspection techniques.

Please contact me directly for more details - if this of interest - since I don't want to sound too much like advertising.

: I am looking for people who deal with the testing of polymeric materials.
: I am interesting in investigation polymers and NDT tests of them.
: Especially rubbers and composites.
: thanks for any help.
: aleks.p.k@iaph.bas-net.by
.
.



 
 Reply 
 
Benmedakhene
Consultant, Consultant on acoustic emission and composites mat
Universite de Technologie de Compiegne, France, Joined Jan 2002, 1

Benmedakhene

Consultant, Consultant on acoustic emission and composites mat
Universite de Technologie de Compiegne,
France,
Joined Jan 2002
1
02:28 May-30-2002
Re: I am looking for people who deal with the testing of polymeric paterials
Our knowledge is in acoustic emission testing of composite materials.
This type of NDT allows a real follow-up of the damage and failure of the composites structures.
If our activity interests you, do not hesitate to contact us.
Universite de Technologie de Compiègne, in France
Cordially


 
 Reply 
 
Jim Knowles
Jim Knowles
03:04 May-30-2002
Re: I am looking for people who deal with the testing of polymeric paterials
: I am looking for people who deal with the testing of polymeric materials.
: I am interesting in investigation polymers and NDT tests of them.
: Especially rubbers and composites.
: thanks for any help.
: aleks.p.k@iaph.bas-net.by
.
.I undertook some ultrasonic inspection work with POLYTEST in Moscow who I believe may be of help.
E-mail:polytest@mtu-net.ru
They have developed inspection methods using ultrasound on PVC and Polythene type plastics.



 
 Reply 
 

Product Spotlight

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window