I am looking for people who deal with the testing of polymeric paterials

I am looking for people who deal with the testing of polymeric materials.
I am interesting in investigation polymers and NDT tests of them.
Especially rubbers and composites.
thanks for any help.
aleks.p.k@iaph.bas-net.by





 
 Reply 
 
Richard Kazares
Richard Kazares
09:13 May-29-2002
Re: I am looking for people who deal with the testing of polymeric paterials
Depending on the specifics of your materials and material geometries, our company has recently introduced a low-frequency based UT technology that can be used to inspect multi-layered, internally bonded, thick-section composites and rubber (also rubber-like) materials from a SINGLE SIDE. The system (which we have named TSCOUT - for Thick Section Composite Oblique Ultrasonic Testing) uses either a single set - or an array (up to 4) sensor pairs at specific angles and frequencies designed to optimize UT penetration (and reflection) form normally VERY DIFFICULT to inspect materials - and which (previously) have almost always required dual-sided (through penetration) inspection techniques.

Please contact me directly for more details - if this of interest - since I don't want to sound too much like advertising.

: I am looking for people who deal with the testing of polymeric materials.
: I am interesting in investigation polymers and NDT tests of them.
: Especially rubbers and composites.
: thanks for any help.
: aleks.p.k@iaph.bas-net.by
.
.



 
 Reply 
 
Benmedakhene
Consultant, Consultant on acoustic emission and composites mat
Universite de Technologie de Compiegne, France, Joined Jan 2002, 1

Benmedakhene

Consultant, Consultant on acoustic emission and composites mat
Universite de Technologie de Compiegne,
France,
Joined Jan 2002
1
02:28 May-30-2002
Re: I am looking for people who deal with the testing of polymeric paterials
Our knowledge is in acoustic emission testing of composite materials.
This type of NDT allows a real follow-up of the damage and failure of the composites structures.
If our activity interests you, do not hesitate to contact us.
Universite de Technologie de Compiègne, in France
Cordially


 
 Reply 
 
Jim Knowles
Jim Knowles
03:04 May-30-2002
Re: I am looking for people who deal with the testing of polymeric paterials
: I am looking for people who deal with the testing of polymeric materials.
: I am interesting in investigation polymers and NDT tests of them.
: Especially rubbers and composites.
: thanks for any help.
: aleks.p.k@iaph.bas-net.by
.
.I undertook some ultrasonic inspection work with POLYTEST in Moscow who I believe may be of help.
E-mail:polytest@mtu-net.ru
They have developed inspection methods using ultrasound on PVC and Polythene type plastics.



 
 Reply 
 

Product Spotlight

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

Teletest Focus+

Teletest Focus+ electronics have superior capabilities than rivals on the market. Beyond the usual
...
test features, Focus+ has 24 transmit channels and 24 receive channels, with an additional on-board switching capabilities. The instrument's frequency range is 10–300 kHz.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window