Inconel 825 Acoustic longitudinal velocity

I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?


 
 Reply 
 
Danny Wang
Danny Wang
09:53 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
: I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
.

John:

Velocity V=D/t Two techniques:
(1)
Find a place with known thickness (t) such as flange.
Using your UT to find the transient time ( delta T). The time from initial pauls to first back wall or the transient time from 1st back wall to 2nd back wall.

V= 2 x thickness/ delta T

(2)
Find a place with known thickness (t) such as flange.
Using your UT, placed a probe on the known thickness area and change the velocity until the first back to the correct thickness.

If you have futher question you can call me at 909-392-5263. or visit my web site at http://www.spectruminspection.org

Danny Wang, PE




 
 Reply 
 
Richard Finlayson
Director, Operations
Princeton Instruments, USA, Joined Jun 2000, 8

Richard Finlayson

Director, Operations
Princeton Instruments,
USA,
Joined Jun 2000
8
00:52 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
: : I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
: .
.
: John:
.
John,

You can find a table of acoustic velocities in Part 2 of the NDT Handbook,UT testing,Volume Seven from ASNT. It shows the longitudinal wave velocity as 5820 m/s for Inconel.

Richard
Major (retired) Richard D. Finlayson
Director, Research, Engineering Applications, Certification,
Training (REACT) and New Business Development
Physical Acoustics Corp.
195 Clarksville Road
Princeton Jct. NJ 08550, USA
Direct Phone: (609)-716-4026
Fax: (609)-716-0706
e-mail: rfinlayson@pacndt.com
web site: www.pacndt.com




 
 Reply 
 
M. W. Moyer
M. W. Moyer
01:41 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
I have the following values for Inconel:
Inconel 600 Inconel
Longitudinal Velocity: 5.915 mm/us 5.820 mm/us
Shear Velocity: 3.078 mm/us 3.020 mm/us
Density: 8.45 gm/cm^3 8.250 gm/cm^3

: I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
.



 
 Reply 
 

Product Spotlight

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window