Inconel 825 Acoustic longitudinal velocity

I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?


 
 Reply 
 
Danny Wang
Danny Wang
09:53 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
: I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
.

John:

Velocity V=D/t Two techniques:
(1)
Find a place with known thickness (t) such as flange.
Using your UT to find the transient time ( delta T). The time from initial pauls to first back wall or the transient time from 1st back wall to 2nd back wall.

V= 2 x thickness/ delta T

(2)
Find a place with known thickness (t) such as flange.
Using your UT, placed a probe on the known thickness area and change the velocity until the first back to the correct thickness.

If you have futher question you can call me at 909-392-5263. or visit my web site at http://www.spectruminspection.org

Danny Wang, PE




 
 Reply 
 
Richard Finlayson
Director, Operations
Princeton Instruments, USA, Joined Jun 2000, 8

Richard Finlayson

Director, Operations
Princeton Instruments,
USA,
Joined Jun 2000
8
00:52 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
: : I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
: .
.
: John:
.
John,

You can find a table of acoustic velocities in Part 2 of the NDT Handbook,UT testing,Volume Seven from ASNT. It shows the longitudinal wave velocity as 5820 m/s for Inconel.

Richard
Major (retired) Richard D. Finlayson
Director, Research, Engineering Applications, Certification,
Training (REACT) and New Business Development
Physical Acoustics Corp.
195 Clarksville Road
Princeton Jct. NJ 08550, USA
Direct Phone: (609)-716-4026
Fax: (609)-716-0706
e-mail: rfinlayson@pacndt.com
web site: www.pacndt.com




 
 Reply 
 
M. W. Moyer
M. W. Moyer
01:41 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
I have the following values for Inconel:
Inconel 600 Inconel
Longitudinal Velocity: 5.915 mm/us 5.820 mm/us
Shear Velocity: 3.078 mm/us 3.020 mm/us
Density: 8.45 gm/cm^3 8.250 gm/cm^3

: I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
.



 
 Reply 
 

Product Spotlight

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>