Technical Discussions
Lotta Inkovaara
R & D
Imatra Steel Oy Ab, Finland, Joined Jun 2002, 1

Lotta Inkovaara

R & D
Imatra Steel Oy Ab,
Finland,
Joined Jun 2002
1
00:07 Jun-10-2002
Immersion ultrasonic testing of steel bars, calibration blocks?

Hello,

I'm a research engineer working on immersion ultrasonic testing of steels. I have three years' experience in testing of square test pieces and now I would like to inspect round bars of 50-140 mm just after rolling. I have already made few test with the tranducer of 10 MHz to diameters of 50-75 mm, but I don't have any specification for the calibration or for the testing. The depth of the testing zone could be 15-20 mm and focal point approximately 10 mm below the surface. The aim is to detect inclusions, so maybe the FBH of 0,5 mm could be useful.

Has somebody already made a specification how to do the calibration and perform the test of round steel bars with immersion method? I would be very glad if somebody could give me advice how to do the calibration and what standard or specification I could use?

Regards,
Lotta inkovaara


 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
02:54 Jun-10-2002
Re: Immersion ultrasonic testing of steel bars, calibration blocks?
Hi,

This test is most common in High Alloy materials used in Control Rods etc in Aviation.

Panametrics has a lot of experience producing Immersion probes with Cylindrical Contour Correction which helps reduce interface ringdown commonly experienced on Bar Stock.

I suggest you contact our office in Waltham ( ndt@panametrics.com ) for further technical assistance.

I have also recently come across an "as-new" set of 4340 and 347SS Convex surface FBH Cal blocks that may be of some use to you, I will send you the details direct.

Regards,

David Hermanutz
Panametrics Melbourne

: Hello,
.
: I'm a research engineer working on immersion ultrasonic testing of steels. I have three years' experience in testing of square test pieces and now I would like to inspect round bars of 50-140 mm just after rolling. I have already made few test with the tranducer of 10 MHz to diameters of 50-75 mm, but I don't have any specification for the calibration or for the testing. The depth of the testing zone could be 15-20 mm and focal point approximately 10 mm below the surface. The aim is to detect inclusions, so maybe the FBH of 0,5 mm could be useful.
.
: Has somebody already made a specification how to do the calibration and perform the test of round steel bars with immersion method? I would be very glad if somebody could give me advice how to do the calibration and what standard or specification I could use?
.
: Regards,
: Lotta inkovaara
.



 
 Reply 
 

Product Spotlight

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window