Lotta Inkovaara
R & D
Imatra Steel Oy Ab, Finland, Joined Jun 2002, 1

Lotta Inkovaara

R & D
Imatra Steel Oy Ab,
Finland,
Joined Jun 2002
1
00:07 Jun-10-2002
Immersion ultrasonic testing of steel bars, calibration blocks?

Hello,

I'm a research engineer working on immersion ultrasonic testing of steels. I have three years' experience in testing of square test pieces and now I would like to inspect round bars of 50-140 mm just after rolling. I have already made few test with the tranducer of 10 MHz to diameters of 50-75 mm, but I don't have any specification for the calibration or for the testing. The depth of the testing zone could be 15-20 mm and focal point approximately 10 mm below the surface. The aim is to detect inclusions, so maybe the FBH of 0,5 mm could be useful.

Has somebody already made a specification how to do the calibration and perform the test of round steel bars with immersion method? I would be very glad if somebody could give me advice how to do the calibration and what standard or specification I could use?

Regards,
Lotta inkovaara


 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
02:54 Jun-10-2002
Re: Immersion ultrasonic testing of steel bars, calibration blocks?
Hi,

This test is most common in High Alloy materials used in Control Rods etc in Aviation.

Panametrics has a lot of experience producing Immersion probes with Cylindrical Contour Correction which helps reduce interface ringdown commonly experienced on Bar Stock.

I suggest you contact our office in Waltham ( ndt@panametrics.com ) for further technical assistance.

I have also recently come across an "as-new" set of 4340 and 347SS Convex surface FBH Cal blocks that may be of some use to you, I will send you the details direct.

Regards,

David Hermanutz
Panametrics Melbourne

: Hello,
.
: I'm a research engineer working on immersion ultrasonic testing of steels. I have three years' experience in testing of square test pieces and now I would like to inspect round bars of 50-140 mm just after rolling. I have already made few test with the tranducer of 10 MHz to diameters of 50-75 mm, but I don't have any specification for the calibration or for the testing. The depth of the testing zone could be 15-20 mm and focal point approximately 10 mm below the surface. The aim is to detect inclusions, so maybe the FBH of 0,5 mm could be useful.
.
: Has somebody already made a specification how to do the calibration and perform the test of round steel bars with immersion method? I would be very glad if somebody could give me advice how to do the calibration and what standard or specification I could use?
.
: Regards,
: Lotta inkovaara
.



 
 Reply 
 

Product Spotlight

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window