7075-T6 Aluminum

I'm looking for the speed of sound in 7075-T6 Aluminum. I would like to get Shear wave, Longitudinal wave and Surface wave velocities if possible.


 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1304

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1304
08:45 Jun-28-2002
Re: 7075-T6 Aluminum
Don:
Dale Ensminger in his textbook published velocity for this aluminium as:
Long.=6350 m/s and Shear = 3100 m/s
(no surface wave value published).

However, discussions with Fred Hotchkiss in Panametrics indicated that some aluminiums may have anisotropy to deal with...

Ed


: I'm looking for the speed of sound in 7075-T6 Aluminum. I would like to get Shear wave, Longitudinal wave and Surface wave velocities if possible.
.



 
 Reply 
 
David Forsyth
R & D
TRI/Austin, USA, Joined Nov 2001, 41

David Forsyth

R & D
TRI/Austin,
USA,
Joined Nov 2001
41
05:51 Jul-04-2002
Re: 7075-T6 Aluminum
Ed is correct, anisotropy in grains due to manufacturing (rolling, extrusion, etc.) can cause measureable differences in velocity in the different directions w.r.t. the processing. I don't know the numbers for Al 7075 off hand. The temper (the T6) is not really important.

Dave.

: Don:
: Dale Ensminger in his textbook published velocity for this aluminium as:
: Long.=6350 m/s and Shear = 3100 m/s
: (no surface wave value published).
.
: However, discussions with Fred Hotchkiss in Panametrics indicated that some aluminiums may have anisotropy to deal with...
.
: Ed
.
:
: : I'm looking for the speed of sound in 7075-T6 Aluminum. I would like to get Shear wave, Longitudinal wave and Surface wave velocities if possible.
: .
.



 
 Reply 
 

Product Spotlight

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window