7075-T6 Aluminum

I'm looking for the speed of sound in 7075-T6 Aluminum. I would like to get Shear wave, Longitudinal wave and Surface wave velocities if possible.


 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1304

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1304
08:45 Jun-28-2002
Re: 7075-T6 Aluminum
Don:
Dale Ensminger in his textbook published velocity for this aluminium as:
Long.=6350 m/s and Shear = 3100 m/s
(no surface wave value published).

However, discussions with Fred Hotchkiss in Panametrics indicated that some aluminiums may have anisotropy to deal with...

Ed


: I'm looking for the speed of sound in 7075-T6 Aluminum. I would like to get Shear wave, Longitudinal wave and Surface wave velocities if possible.
.



 
 Reply 
 
David Forsyth
R & D
TRI/Austin, USA, Joined Nov 2001, 41

David Forsyth

R & D
TRI/Austin,
USA,
Joined Nov 2001
41
05:51 Jul-04-2002
Re: 7075-T6 Aluminum
Ed is correct, anisotropy in grains due to manufacturing (rolling, extrusion, etc.) can cause measureable differences in velocity in the different directions w.r.t. the processing. I don't know the numbers for Al 7075 off hand. The temper (the T6) is not really important.

Dave.

: Don:
: Dale Ensminger in his textbook published velocity for this aluminium as:
: Long.=6350 m/s and Shear = 3100 m/s
: (no surface wave value published).
.
: However, discussions with Fred Hotchkiss in Panametrics indicated that some aluminiums may have anisotropy to deal with...
.
: Ed
.
:
: : I'm looking for the speed of sound in 7075-T6 Aluminum. I would like to get Shear wave, Longitudinal wave and Surface wave velocities if possible.
: .
.



 
 Reply 
 

Product Spotlight

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window