Look for under ground pipeline corrosion inspection system

Dear all:
I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!


 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:46 Jan-15-2002
Re: Look for under ground pipeline corrosion inspection system
You can contact No Pig at Email fino@finoag.com

Mark your email for the attention of Michael Broderick.

Their tel number is +49 5063 9599

WE have been looking at No Pig a lot plus other underground inspection techniques. If you need assistance please feel free to contact me direct.


 
 Reply 
 
Brant Shields
Brant Shields
08:16 Feb-20-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!
.

Have you considered Guided Ultrasonics for your underground piping? Contact us for any information or questions you may have.


 
 Reply 
 
Peter
Consultant
PQS, United Kingdom, Joined Jan 2002, 7

Peter

Consultant
PQS,
United Kingdom,
Joined Jan 2002
7
08:11 Feb-21-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!

Guided Ultrasonics Ltd manufacture Wavemaker SE16 guided wave pipe screening system which is in use worldwide. Look at website www.guided-ultrasonics.com or contact Peter@guided-ultrasonics.com for more info.



 
 Reply 
 
Jim Yukes
Jim Yukes
09:29 Feb-22-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!
.
Can you give more information about the pipe to be inspected? We can supply an electromagnetic system for small diameter pipes and may be able to do something for larger diameters depending on the length of the line. Do you have access to the pipe OD? E-Pit will inspect from the OD through coatings. See : www.russelltech.com


 
 Reply 
 
Jim Yukes
Jim Yukes
09:29 Feb-22-2002
Re: Look for under ground pipeline corrosion inspection system
: Dear all:
: I am look for under ground pipeline corrosion inspection system.especially no pig system. please help me!
.
Can you give more information about the pipe to be inspected? We can supply an electromagnetic system for small diameter pipes and may be able to do something for larger diameters depending on the length of the line. Do you have access to the pipe OD? E-Pit will inspect from the OD through coatings. See : www.russelltech.com


 
 Reply 
 
Jamie Gauthier
Jamie Gauthier
00:45 Feb-22-2002
Re: Look for under ground pipeline corrosion inspection system
We have a system that can determine underground corrosion. Please call RTD Quality Services Inc. for further details.

Toll Free: 800-661-0066
Reception: 780-440-6600
Fax: 780-440-2538
Web: www.rtdquality.com
Email: jgauthier@rtdquality.com


 
 Reply 
 
David
David
06:09 Feb-25-2002
Re: Look for under ground pipeline corrosion inspection system
We are from a third party inspection company having international operation. We provide one-stop NDT solutions for the oil and gas pipeline inspections.

We are able to inspect for underground pipeline inspection without the need to remove insulation (dig)or pigging up to 100 metres depending on the anticipated condition of the pipe. Only one spot for each measurement is required at exposed areas like road crossing etc. The equipment we are using is sophisticated and reliable.

Other services available include corrosion under insulation (CUI) inspection where the need to remove insulation (up to 150 mm) is eliminated.

Kindly furnish us with more info on the pipeline i.e. ID, OD, length, base material, drawings (if necessary) for us to evaluate the situation and provide you the appropriate solution for your attention.

Rgds, David.


 
 Reply 
 
Musarrat Imam
Musarrat Imam
03:18 Jul-02-2002
Re: Look for under ground pipeline corrosion inspection system
We have a pipe sea water under ground carbonsteel pipe 72 and 84" dia. The pipe is corroded externally. The pipe is protected inside by glassflaking and externally hot applied bitumen membrane. we want to refurbish the pipe externally online inorder to withstand the pipe 10-15 years. The pipe was laid in 1970. please advise
1. do you have any technology which can find out the corrosion precentage of the pipe.
2. What kind of coating you will prefer to protect the pipe.

regards,
M.imam
mimam@qafco.com.qa


 
 Reply 
 
Bhaskar
Bhaskar
11:44 Dec-14-2010
Re: Look for under ground pipeline corrosion inspection system
In Reply to David at 06:09 Feb-25-2002 .

We would like to know the system for wall thickness measurement of underground pipeline without exposure to outside (ie burried pipeline of 1 to 2 KM) Dia ranges from small to Big.

 
 Reply 
 

Product Spotlight

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

NovaScope 6000

The all-digital Novascope 6000 is a portable, ultra-high precision thickness gauge for high-speed
...
thickness measurement. Novascope 6000 has unmatched capabilities and unique features including: •Superior Resolution with high contrast, high-speed color RF display •High pulser voltage •Real-time video output •Increased internal/external data storage •Programmable SetUp features •Battery & AC Powered
>

Share...