03:28 Jul-15-2002
tube-to-tubesheet weld scanner

I´m looking for an ultrasonic tube-to-tubesheet weld scanner
or an UT inspection system with remote scanner to inspect tube-to-
tubesheet welds for pores with pores size >0.5 mm and for lack of
fusion. To be inspected are welds with tube excess out of tubesheet
of some mm.


 
 Reply 
 
Charlie Jackson
NDT Inspector
Northern.NDT.services LTD, United Kingdom, Joined Oct 1999, 1

Charlie Jackson

NDT Inspector
Northern.NDT.services LTD,
United Kingdom,
Joined Oct 1999
1
09:52 Jul-16-2002
Re: tube-to-tubesheet weld scanner
: I´m looking for an ultrasonic tube-to-tubesheet weld scanner
: or an UT inspection system with remote scanner to inspect tube-to-
: tubesheet welds for pores with pores size >0.5 mm and for lack of
: fusion. To be inspected are welds with tube excess out of tubesheet
: of some mm.
.
Dear Peter
Some years ago the Force Institute in Broenby Denmark were performing such work, they would be worth a call. Contacts are Hans Ole Olsen or Yens Grassov
Regards Charlie



 
 Reply 
 
Massimo Carminati
Massimo Carminati
06:46 Jul-18-2002
Re: tube-to-tubesheet weld scanner
We have designed and engineered several of this manipulators (manual or motorized)for heat exchangers manufacturers with or without UT system with B and C-Scan presentation according to the Stamicarbon rules.

Feel free to contact me.



 
 Reply 
 
Leif Jeppesen
R & D
FORCE Technology, Denmark, Joined Nov 1998, 6

Leif Jeppesen

R & D
FORCE Technology,
Denmark,
Joined Nov 1998
6
07:56 Jul-18-2002
Re: tube-to-tubesheet weld scanner
: I´m looking for an ultrasonic tube-to-tubesheet weld scanner
: or an UT inspection system with remote scanner to inspect tube-to-
: tubesheet welds for pores with pores size >0.5 mm and for lack of
: fusion. To be inspected are welds with tube excess out of tubesheet
: of some mm.
.
FORCE Technology has developed the AHS-1 scanner for the P-scan System 4 for inspection of tube-to-tube sheet welds. The scanner can inspect up to 3 welds in parallel and the data acquisition is controlled directly from the scanner. Inspection speed is up to 300 welds per hour. For further information please look under brochures at www.p-scan.com


 
 Reply 
 
Randy Plis
Sales, Consultant
AMDATA NDE Technology LLC, USA, Joined Oct 1999, 23

Randy Plis

Sales, Consultant
AMDATA NDE Technology LLC,
USA,
Joined Oct 1999
23
08:40 Jul-22-2002
Re: tube-to-tubesheet weld scanner
We also have a tube-to-sheet scanner as an available accessory for our IntraSpect UT C-Scan imaging systems. Such a scanner has been used to inspect near drums in fossil boilers, as well as reactor and pressurizer penetrations in nuclear applications. Please contact us to provide additional detials.

Best regards,
Randy Plis


 
 Reply 
 
Jeff Kott
Jeff Kott
02:30 Jul-30-2002
Re: tube-to-tubesheet weld scanner
: I´m looking for an ultrasonic tube-to-tubesheet weld scanner
: or an UT inspection system with remote scanner to inspect tube-to-
: tubesheet welds for pores with pores size >0.5 mm and for lack of
: fusion. To be inspected are welds with tube excess out of tubesheet
: of some mm.
.

We have an OmniScan system that is capable of such inspections. You can contact me if you have any further questions.


 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window