I´m looking for an ultrasonic tube-to-tubesheet weld scanner
or an UT inspection system with remote scanner to inspect tube-to-
tubesheet welds for pores with pores size >0.5 mm and for lack of
fusion. To be inspected are welds with tube excess out of tubesheet
of some mm.


 
 Reply 
 
Charlie Jackson
NDT Inspector
Northern.NDT.services LTD, United Kingdom, Joined Oct 1999, 1

Charlie Jackson

NDT Inspector
Northern.NDT.services LTD,
United Kingdom,
Joined Oct 1999
1
09:52 Jul-16-2002
Re: tube-to-tubesheet weld scanner
: I´m looking for an ultrasonic tube-to-tubesheet weld scanner
: or an UT inspection system with remote scanner to inspect tube-to-
: tubesheet welds for pores with pores size >0.5 mm and for lack of
: fusion. To be inspected are welds with tube excess out of tubesheet
: of some mm.
.
Dear Peter
Some years ago the Force Institute in Broenby Denmark were performing such work, they would be worth a call. Contacts are Hans Ole Olsen or Yens Grassov
Regards Charlie



 
 Reply 
 
Massimo Carminati
Massimo Carminati
06:46 Jul-18-2002
Re: tube-to-tubesheet weld scanner
We have designed and engineered several of this manipulators (manual or motorized)for heat exchangers manufacturers with or without UT system with B and C-Scan presentation according to the Stamicarbon rules.

Feel free to contact me.



 
 Reply 
 
Leif Jeppesen
R & D
FORCE Technology, Denmark, Joined Nov 1998, 6

Leif Jeppesen

R & D
FORCE Technology,
Denmark,
Joined Nov 1998
6
07:56 Jul-18-2002
Re: tube-to-tubesheet weld scanner
: I´m looking for an ultrasonic tube-to-tubesheet weld scanner
: or an UT inspection system with remote scanner to inspect tube-to-
: tubesheet welds for pores with pores size >0.5 mm and for lack of
: fusion. To be inspected are welds with tube excess out of tubesheet
: of some mm.
.
FORCE Technology has developed the AHS-1 scanner for the P-scan System 4 for inspection of tube-to-tube sheet welds. The scanner can inspect up to 3 welds in parallel and the data acquisition is controlled directly from the scanner. Inspection speed is up to 300 welds per hour. For further information please look under brochures at www.p-scan.com


 
 Reply 
 
Randy Plis
Sales, Consultant
AMDATA NDE Technology LLC, USA, Joined Oct 1999, 23

Randy Plis

Sales, Consultant
AMDATA NDE Technology LLC,
USA,
Joined Oct 1999
23
08:40 Jul-22-2002
Re: tube-to-tubesheet weld scanner
We also have a tube-to-sheet scanner as an available accessory for our IntraSpect UT C-Scan imaging systems. Such a scanner has been used to inspect near drums in fossil boilers, as well as reactor and pressurizer penetrations in nuclear applications. Please contact us to provide additional detials.

Best regards,
Randy Plis


 
 Reply 
 
Jeff Kott
Jeff Kott
02:30 Jul-30-2002
Re: tube-to-tubesheet weld scanner
: I´m looking for an ultrasonic tube-to-tubesheet weld scanner
: or an UT inspection system with remote scanner to inspect tube-to-
: tubesheet welds for pores with pores size >0.5 mm and for lack of
: fusion. To be inspected are welds with tube excess out of tubesheet
: of some mm.
.

We have an OmniScan system that is capable of such inspections. You can contact me if you have any further questions.


 
 Reply 
 

Product Spotlight

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window