03:34 Aug-12-2002
Thickness measurement

Hello everybody.
May somebody help me?
I need measure thickness of pipewall but I have one trouble.
Diameter of pipeline is 2500mm, and thickness of pipe wall is about 6-10mm.
I have apparatus DM-2LCDM with transducer DA211.
And what trouble?
This pipe is in blast furnance. Its leaning gas tubing.Entrance to the pipeline is only from one side(from above), and is impossible go round all pipe because its much high(60m).But I need measure all surface, but my hand is too short.(diameter 2500mm). Do you know how can I solve this trouble?
Thank you.
Milan
Sorry for my poor english.


 
 Reply 
 
Richard Kazares
Richard Kazares
06:44 Aug-12-2002
Re: Thickness measurement
You have an interesting problem - and I think we have a good solution for you - we manufacture a CONFIGURABLE magnetic scanner - that can easly go around the inside of a 2500 mm pipe - and perform a 100% thickness survery for you.

If you follow the link below to our website and get information on LSI (Large Structure Inspection) System.

It would be more than likely that we can help you perform this test - we have systems available for use in North America (4 systems), Europe (4 systems), the Middle East (1 system), South America (2 systems) and Japan (1 system).

Alternatively, you may contact me directly for more information.

Richard Kazares
General Manager
NDT Automation
1-619-716-4123

: Hello everybody.
: May somebody help me?
: I need measure thickness of pipewall but I have one trouble.
: Diameter of pipeline is 2500mm, and thickness of pipe wall is about 6-10mm.
: I have apparatus DM-2LCDM with transducer DA211.
: And what trouble?
: This pipe is in blast furnance. Its leaning gas tubing.Entrance to the pipeline is only from one side(from above), and is impossible go round all pipe because its much high(60m).But I need measure all surface, but my hand is too short.(diameter 2500mm). Do you know how can I solve this trouble?
: Thank you.
: Milan
: Sorry for my poor english.
.



 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
07:30 Aug-13-2002
Re: Thickness measurement
From what Mr.Milan wrote, I got the impression that he cannot access the ID of the pipe, but can access the pipe only from OD and that too from above. In such a case, a magnetic crawler or a ring with the probe mounted by a spring so that contact is assured can be tried.

If he clarifies the access (from OD or ID), the solutions can be thought of.


: You have an interesting problem - and I think we have a good solution for you - we manufacture a CONFIGURABLE magnetic scanner - that can easly go around the inside of a 2500 mm pipe - and perform a 100% thickness survery for you.
.
: If you follow the link below to our website and get information on LSI (Large Structure Inspection) System.
.
: It would be more than likely that we can help you perform this test - we have systems available for use in North America (4 systems), Europe (4 systems), the Middle East (1 system), South America (2 systems) and Japan (1 system).
.
: Alternatively, you may contact me directly for more information.
.
: Richard Kazares
: General Manager
: NDT Automation
: 1-619-716-4123
.
.
: : Hello everybody.
: : May somebody help me?
: : I need measure thickness of pipewall but I have one trouble.
: : Diameter of pipeline is 2500mm, and thickness of pipe wall is about 6-10mm.
: : I have apparatus DM-2LCDM with transducer DA211.
: : And what trouble?
: : This pipe is in blast furnance. Its leaning gas tubing.Entrance to the pipeline is only from one side(from above), and is impossible go round all pipe because its much high(60m).But I need measure all surface, but my hand is too short.(diameter 2500mm). Do you know how can I solve this trouble?
: : Thank you.
: : Milan
: : Sorry for my poor english.
: .
.



 
 Reply 
 

Product Spotlight

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>