Dear,
Can any one tell UT as per ASTM-578 which acceptance criteria is more straingent either LEVEL B or LEVEL C?

 
 Reply 
 
GP
Engineering
India, Joined Sep 2009, 2

GP

Engineering
India,
Joined Sep 2009
2
14:31 Oct-28-2009
Re: NDT: SA 578- LEVEL B & C
In Reply to Dhaval Patel at 06:14 Oct-28-2009 (Opening).

Level C is more stringent compared to level B.As per level C,more than 1" continous total loss of back wall reflection plates are rejected.

 
 Reply 
 
Dhaval J patel
Dhaval J patel
04:19 Oct-29-2009
Re: NDT: SA 578- LEVEL B & C
Ref. to my earlier query
Plates acctedpted by Level C can be certified as Level B?
 
 Reply 
 
GP
Engineering
India, Joined Sep 2009, 2

GP

Engineering
India,
Joined Sep 2009
2
09:02 Oct-29-2009
Re: NDT: SA 578- LEVEL B & C
In Reply to Dhaval J patel at 04:19 Oct-29-2009 .

Yes,you can certify as level B.

 
 Reply 
 
CIRO SANTOMARTINO
NDT Inspector,
D.e M.I. srl, Italy, Joined Oct 2009, 86

CIRO SANTOMARTINO

NDT Inspector,
D.e M.I. srl,
Italy,
Joined Oct 2009
86
17:20 Oct-29-2009
Re: NDT: SA 578- LEVEL B & C
In Reply to Dhaval Patel at 06:14 Oct-28-2009 (Opening).

level c. is more straingent .

 
 Reply 
 
R. BALAKUMAR
R. BALAKUMAR
07:02 Nov-14-2012
Re: NDT: SA 578- LEVEL B & C
In Reply to CIRO SANTOMARTINO at 17:20 Oct-29-2009 .

Dear sir,
ASTM A 578 level C or B which is equilent to EN 10160 S1 E1

 
 Reply 
 

Product Spotlight

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window