Eddy current testing for welds

Hi everyone,
I have quick questions related to Weld Eddy Current Tesing:
1. " When we use 100kHz probe, Can we detect subsurface defects within 2mm depth? because we used the calibration block with 2mm depth slot signal is reference level (eg. 80% of full screen)?
2. With the thin thickness of parent metal in weld testing will affect to the ECT signal? and How to control if YES?
Eg: the weld with the parent metal thickness is 2 or 3mm whilst we us ED slot calibration block with 5mm thick.
Thanks

 
 Reply 
 
John Hansen
Director, - Eddy Current Technology
ETher NDE Ltd, United Kingdom, Joined Oct 1999, 73

John Hansen

Director, - Eddy Current Technology
ETher NDE Ltd,
United Kingdom,
Joined Oct 1999
73
10:32 Dec-06-2012
Re: Eddy current testing for welds
In Reply to creed at 04:48 Dec-06-2012 (Opening).

1) At 100 kHz in Carbon Steel (Ferromagnetic) the Standard Depth of Penetration (aka skin depth) is about 0.03 mm. This means that as standard then eddy current can only be considered a surface method.

2) I think your question is now answered unless your material is non-magnetic.

All the best

John Hansen

1
 
 Reply 
 
Franlk Lund
R & D,
United Kingdom, Joined Apr 2005, 221

Franlk Lund

R & D,
United Kingdom,
Joined Apr 2005
221
11:45 Dec-06-2012
Re: Eddy current testing for welds
In Reply to creed at 04:48 Dec-06-2012 (Opening).

Creed,

1. The calibration slot starts from the inspection surface, so it gives a path for the interrogating current to penetrate into the test block by going down and up the flanks of the slot. If your slot is on the other side of the block, then the interrogating current in the slotless surface is not interrupted and will not see the slot.

2. Things get different when your 2mm deep vertical slot penetrates to the other side of the 2mm thick test piece. Of course, a slanted defect can have a 2mm pocket depth without penetrating a 2mm thick plate.

Cheers,
Frank

 
 Reply 
 
creed
NDT Inspector,
n.n., Joined Jul 2009, 33

creed

NDT Inspector,
n.n.,
Joined Jul 2009
33
22:41 Dec-06-2012
Re: Eddy current testing for welds
In Reply to John Hansen at 10:32 Dec-06-2012 .

Thanks John and Franlk.
Your answers make me feel open-minded. Prior I had stupid perpective in checking thin material might affected to signal.
Cheers.

 
 Reply 
 

Product Spotlight

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

MIZ®-21C: Truly Affordable Eddy Current Handheld with Surface Array Capability

Introducing MIZ-21C, the first truly affordable handheld eddy current instrument with surface array
...
capabilities. MIZ-21C can deliver fast, accurate inspections in demanding NDT applications including aerospace, oil and gas, manufacturing, and power generation. The surface array solution can reduce inspection time by up to 95% compared to traditional handheld pencil probes. The ergonomic design, long battery life, and intuitive touchscreen mean you can inspect more areas faster than ever without fatigue.
>

NovaScope 6000

The all-digital Novascope 6000 is a portable, ultra-high precision thickness gauge for high-speed
...
thickness measurement. Novascope 6000 has unmatched capabilities and unique features including: •Superior Resolution with high contrast, high-speed color RF display •High pulser voltage •Real-time video output •Increased internal/external data storage •Programmable SetUp features •Battery & AC Powered
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>