Folks,

I am wondering if anyone can reference me to information regarding surface preparation of an EDM cut aluminum surface that is to be penetrant inspected. My concerns are whether etching should be required or not, if so how aggressive of an etch, if not is there a different surface prep that is recommended. Does the EDM process have the tendency to smear metal, close pre-existing discontinuities, create new discontinuities?

I am not familiar with the EDM process, therefore I have more questions than answers at this point and would appreciate any input from anyone who does have some experience.

Thanks in advance for your time,

Brian Younce
NDT Level III
Hartzell Propeller Inc.



 
 Reply 
 
Phil Herman Jr.
Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards, USA, Joined Oct 1999, 79

Phil Herman Jr.

Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards,
USA,
Joined Oct 1999
79
01:15 Oct-09-2002
Re: Pre-penetrant Surface Prep of an EDM Cut Aluminum Surface
Brian,

PH Tool Reference Standards manufactures EDM notch standards and test blocks for all NDT disciplines. While we are most familiar with the "micro-machining" of narrow notches and slots, we also perform both conventional (a.k.a. sinker) and wire EDM. It would be helpful to know which process was used to manufacture the aluminum parts you need to PT. Feel free to contact me directly at 888-553-9245 or philjr@phtool.com.

Phil Herman Jr.
PH Tool


: Folks,
.
: I am wondering if anyone can reference me to information regarding surface preparation of an EDM cut aluminum surface that is to be penetrant inspected. My concerns are whether etching should be required or not, if so how aggressive of an etch, if not is there a different surface prep that is recommended. Does the EDM process have the tendency to smear metal, close pre-existing discontinuities, create new discontinuities?
.
: I am not familiar with the EDM process, therefore I have more questions than answers at this pointand would appreciate any input from anyone who does have some experience.
.
: Thanks in advance for your time,
.
: Brian Younce
: NDT Level III
: Hartzell Propeller Inc.
.



 
 Reply 
 
Sergio Bilbao
Sergio Bilbao
01:29 Oct-09-2002
Re: Pre-penetrant Surface Prep of an EDM Cut Aluminum Surface

Brian,

It depends on how your EDM Process in made.
For example, the roughness you are achieving. Anyway, EDM machined surfaces have a surface quality quite good.
If you are going to make a sensitivity 2 FP Inspection, it is probably you will get an acceptable background.

The EDM's most important characteristic is that it modifies the grain size in the subsurface layer, known as "Recast Layer". But it is not important for the FPI.

The EDM does not close discontinuities. And generally, doesn't create news indications.

Be care of oxidations and burns.

Regards.


: Folks,
.
: I am wondering if anyone can reference me to information regarding surface preparation of an EDM cut aluminum surface that is to be penetrant inspected. My concerns are whether etching should be required or not, if so how aggressive of an etch, if not is there a different surface prep that is recommended. Does the EDM process have the tendency to smear metal, close pre-existing discontinuities, create newdiscontinuities?
.
: I am not familiar with the EDM process, therefore I have more questions than answers at this point and would appreciate any input from anyone who does have some experience.
.
: Thanks in advance for your time,
.
: Brian Younce
: NDT Level III
: Hartzell Propeller Inc.
.



 
 Reply 
 

Product Spotlight

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window