Ch.Y.Xiao
Ch.Y.Xiao
04:11 Jun-22-2002
About metal hardness testing by eddy-current

Who can give me some suggestions about metal hardness testing by eddy-current?
Thanks.


 
 Reply 
 
S.V.Swamy
Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex , India, Joined Feb 2001, 787

S.V.Swamy

Engineering, - Material Testing Inspection & Quality Control
Retired from Nuclear Fuel Complex ,
India,
Joined Feb 2001
787
03:47 Jun-23-2002
Re: About metal hardness testing by eddy-current
: Who can give me some suggestions about metal hardness testing by eddy-current?
: Thanks.

Pl. describe clearly what you are looking for. If you prefer, you can contact me directly at .

Swamy



 
 Reply 
 
Sean Franklin
Sean Franklin
06:52 Jun-24-2002
Re: About metal hardness testing by eddy-current
:In addition to eddy-current, Resistivity – a basic principle of electricity - is a proven and widely used method of ndt to help determine the case depth and hardness of metal. The Physical Acoustics M100A Metal Inspector uses resistivity as it pulses a rapidly reversing direct current into the metal through a 4-point probe, and measures the metal’s resistance to the current flow.

Metal in a hardened state will always exhibit a higher resistivity to the flow of electricity than an unhardened metal because its grain structure has become more tightly packed through heat treatment. The greater the case depth of any given parts, the higher the resistivity reading on the M100A display screen. Likewise, annealing will bring the resistivity back down.

For further information, please contact Sean Franklin at Physical Acoustics Corporation, via Sfranklin@PACNDT.com or (609) 716-4088

: Who can give me some suggestions about metal hardness testing by eddy-current?
: : Thanks.
.
: Pl. describe clearly what you are looking for. If you prefer, you can contact me directly at .
.
: Swamy
.



 
 Reply 
 
David Forsyth
R & D
TRI/Austin, USA, Joined Nov 2001, 41

David Forsyth

R & D
TRI/Austin,
USA,
Joined Nov 2001
41
06:09 Jul-04-2002
Re: About metal hardness testing by eddy-current
Conductivity/resistivity measurements are not able to determine hardness in 7000 series aluminiums, see
http://www.ndt.net/article/aero1197/forsyth/forsyth.htm Figure 1, which should have an x axis label of conductivity. I do not know about other materials.

Dave.

: :In addition to eddy-current, Resistivity – a basic principle of electricity - is a proven and widely used method of ndt to help determine the case depth and hardness of metal.


 
 Reply 
 
SADIK SAYYED
SADIK SAYYED
08:55 Oct-12-2002
Re: About metal hardness testing by eddy-current and experimental set up for the same
: Conductivity/resistivity measurements are not able to determine hardness in 7000 series aluminiums, see
: http://www.ndt.net/article/aero1197/forsyth/forsyth.htm Figure 1, which should have an x axis label of conductivity. I do not know about other materials.
.
: Dave.
.
: : :In addition to eddy-current, Resistivity – a basic principle of electricity - is a proven and widely used method of ndt to help determine the case depth and hardness of metal. also tell me about experimental setup to determine the hardness by this method .

.



 
 Reply 
 

Product Spotlight

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window