Taking thickness readings on FRP material.

I would like to find out if there is such a thing as a, UT transducer, that is able to take thickness readings of FRP pipe material. (* FRP = Fiber Reinforced Plastic *)

I don't think that a transducer would be able to use sound to obtain a thickness reading due to the amout of glass fiber in the material. But then again, I could be completely wrong and need to be shown the light.

Thanks,
K Fosha


 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 159

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
159
06:28 Dec-18-2002
Re: Taking thickness readings on FRP material.
: I would like to find out if there is such a thing as a, UT transducer, that is able to take thickness readings of FRP pipe material. (* FRP = Fiber Reinforced Plastic *)
.
: I don't think that a transducer would be able to use sound to obtain a thickness reading due to the amout of glass fiber in the material. But then again, I could be completely wrong and need to be shown the light.
.
: Thanks,
: K Fosha
.
Over the years I have had a number of experiences with FRP. Krautkramer once had a thickness gauge the CL202F which uses the ZIP zero interface probe, it is now no longer available. This probe works well as it is a 0.5MHz probe with a special delay block to reduce the interface echo, ( as the name implies). Details can be found on the KK website about ZIP probes.

Recently we have been using the piezo-composite probes for testing FRP pipe and rubber conveyor belt with great success. Try the K1SC, MSEK2 and MK1S

Regards

Neil Burleigh


 
 Reply 
 
Taha R Sheikh
Taha R Sheikh
18:01 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to Neil Burleigh at 06:28 Dec-18-2002 .

hello neil,

i just read ur reply below.

unfortuatly i cant get any of the below mentioned products in KK website.
Please send me the link or advice me accordingly for thickness montioring of FRP ducts!

taha

 
 Reply 
 
Sudheer Jai Krishnan
Sudheer Jai Krishnan
21:01 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to Taha R Sheikh at 18:01 Feb-28-2013 .

Hello Taha

Please let us know your min and maximum thickness. Have you tried a 45MG or a 38DL Plus for the thickness measurements? If not please see the link below and We have given solutions for similar kind of application to many of our customers. The highlighting feature is that ,the 38DLP has got both precision thickness measurements and corrosion measurements such that you can have one equipment for your different requirements

Kindly let me know if i can be of any assistance to you.

http://www.olympus-ims.com/en/38dl-plus/

Regards

Sudheer Jai Krishnan

 
 Reply 
 
James Scalf
NDT Inspector,
Global Integrity, Canada, Joined Oct 2012, 274

James Scalf

NDT Inspector,
Global Integrity,
Canada,
Joined Oct 2012
274
21:04 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to Sudheer Jai Krishnan at 21:01 Feb-28-2013 .

Taha,

Another option is the new Zip line of probes available through General Electric... Check online to find a representative near you...

 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
21:06 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to K Fosha at 02:14 Dec-17-2002 (Opening).

Yes, there are transducers suitable for fiberglass testing. For more than 25 years Panametrics and now Olympus NDT has offered a specialized 500 KHz delay line transducer, the M2008, that is optimized for thickness measurement and detection of laminar flaws in fiberglass up to 100 mm or thicker. It uses an impedance matched delay line for good coupling and minimal interface echo interference. It can be used with high penetration thickness gages or with a flaw detector. The application note in the link below references fiberglass boat hulls, but the principle is applicable to fiberglass pipes as well.

http://www.olympus-ims.com/en/applications/thickness-gaging-fiberglass-boat-hulls/

We (and other major manufacturers as well) also offer a number of other low frequency transducers that can be effectively used on fiberglass in various thickness ranges. If your pipe radius is less than approximately 150 mm we would first try a smaller diameter transducer as an alternative, such as a 1 MHz or 2.25 MHz, 12.5 mm diameter broadband contact transducer.

 
 Reply 
 

Product Spotlight

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window