02:25 Nov-02-2002
co2 Pitting 13 Chrome

I am trying to find out if anyone has had much experience with find CO2 pitting on 13 chrome material in full lengths of pipe and the method used to detect that pitting. I have about 16000 feet of pipe to look at with minor pitting .017" to .060" and I am having trouble with my signal to noise ratio just wondering if anyone out there knows or can help with this situation?


 
 Reply 
 
Richard D. Roberts
Engineering, Executive Managment
Quest Integrity Group, USA, Joined Nov 1998, 78

Richard D. Roberts

Engineering, Executive Managment
Quest Integrity Group,
USA,
Joined Nov 1998
78
00:13 Nov-04-2002
Re: co2 Pitting 13 Chrome
Ed,

Have you considered using LASER NDT to inspect the piping? The Laser-Optic Tube Inspection (LOTIS) process can reliably detect and quantify pitting with depths as shallow as +/-0.002" and pit diameters as small as 0.005". Currently there are laser probes built which can inspect piping up to 5.4" ID. Not sure what size your piping is?

For more information you might want to take a look at our web-site which can be found at http://www.qi2.com/field/fsddef.htm

If you have any further questions please contact me at the numbers listed below.

Regards,

Richard D. Roberts
V.P. Field Services
QUEST Integrated, Inc.
1012 Central Avenue South
Kent, Washington 98032 USA

Direct Tel: 1-253 872-9500 ext. 1275
Toll Free Tel: 1-800 233-3345 ext. 1275
Cell: 1-206 571-4302
Fax: 1-253-872-8967
Email: richardr@qi2.com
Web Site: http://www.qi2.com/field/fsddef.htm

-------------- ORIGIONAL MESSAGE ----------------
: I am trying to find out if anyone has had much experiencewith find CO2 pitting on 13 chrome material in full lengths of pipe and the method used to detect that pitting. I have about 16000 feet of pipe to look at with minor pitting .017" to .060" and I am having trouble with my signal to noise ratio just wondering if anyone out there knows or can help with this situation?



 
 Reply 
 

Product Spotlight

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

SONOAIR - air-coupled Phased Array Ultrasonic Inspection System

For highly attenuating materials, the performance of the system is critical. The ultrasonic sensors,
...
the scanning area and the system settings should be flexibly adapted to the test task and the material. These high expectations are met with the new and modular testing system SONOAIR. With the world’s first air-coupled phased-array UT inspection system SONOAIR we developed a technology that works with up to 4 transmitter and receiver channels with freely configurable square wave burst transmitters as wells as low noise receiving amplifiers.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

NovaScope 6000

The all-digital Novascope 6000 is a portable, ultra-high precision thickness gauge for high-speed
...
thickness measurement. Novascope 6000 has unmatched capabilities and unique features including: •Superior Resolution with high contrast, high-speed color RF display •High pulser voltage •Real-time video output •Increased internal/external data storage •Programmable SetUp features •Battery & AC Powered
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window