ismail sarpun
ismail sarpun
02:26 Nov-06-2002
experimetal setup

I want to establish a system which I can determine grain size. so is there anyone can help me?


 
 Reply 
 
DJ Kallhof
DJ Kallhof
04:38 Nov-07-2002
Re: experimetal setup
: I want to establish a system which I can determine grain size. so is there anyone can help me?
.
Polishing the material to a mirror finish, followed by a chemical etch, will reveal the grain sufficiently to observe with proper magnification. A permanent record may be obtained by replicating the surface. Respond back with the material you are working with.


 
 Reply 
 
Scott Longstreet
NDT Inspector, Metallographer
Areospace, USA, Joined Apr 2002, 5

Scott Longstreet

NDT Inspector, Metallographer
Areospace,
USA,
Joined Apr 2002
5
05:21 Nov-07-2002
Re: experimetal setup
: : I want to establish a system which I can determine grain size. so is there anyone can help me?
: .
: Polishing the material to a mirror finish, followed by a chemical etch, will reveal the grain sufficiently to observe with proper magnification. A permanent record may be obtained by replicating the surface. Respond back with the material you are working with.
.
ASTM E8 Would be an excellent refernece guide!


 
 Reply 
 
Scott Longstreet
Scott Longstreet
06:29 Nov-07-2002
Re: experimetal setup
: I want to establish a system which I can determine grain size. so is there anyone can help me?
.
Soory, I meant to suggest ASTM E3 as a guide. For that matter, look into the many ASTM standars for help.


 
 Reply 
 

Product Spotlight

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window