John carpenter
John carpenter
21:08 Aug-11-2013
Wire IQI

Hello everyoane,
How you calculate the radiographic sensitivity when using the wire IQI.I only used the hole type penetrameters, but now there s a European customer that want us to use the wire type.I know there are some standards out there, but maybe somebody can explain it to me much clearer.Thank you

 
 Reply 
 
andrew cunningham
NDT Inspector
Canada, Joined Jun 2008, 238

andrew cunningham

NDT Inspector
Canada,
Joined Jun 2008
238
23:30 Aug-11-2013
Re: Wire IQI
In Reply to John carpenter at 21:08 Aug-11-2013 (Opening).

If you are shooting through 100mm of steel and you can see a IQI 1mm wire. I would think you would have 1% But I could be wrong.

 
 Reply 
 
John carpenter
John carpenter
23:42 Aug-11-2013
Re: Wire IQI
In Reply to andrew cunningham at 23:30 Aug-11-2013 .

Thank you for your answer, but I think there s a formula that need to be applied based on the thinnest wire visible.Anyway if somebody have experience working with this type of IQI please give me some feedback.

 
 Reply 
 
Ed T.
Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III, Saudi Arabia, Joined Sep 2011, 169

Ed T.

Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III,
Saudi Arabia,
Joined Sep 2011
169
08:12 Aug-12-2013
Re: Wire IQI
In Reply to John carpenter at 23:42 Aug-11-2013 .

I believe this is correct.

Calculate the radiographic sensitivity for a wire-type penetrameter using the formula:

Sensitivity (%) = Thickness of the thinnest wire * 100/Specimen thickness

 
 Reply 
 
shahid
NDT Inspector,
Pakistan, Joined Mar 2013, 10

shahid

NDT Inspector,
Pakistan,
Joined Mar 2013
10
13:49 Aug-12-2013
Re: Wire IQI
In Reply to John carpenter at 21:08 Aug-11-2013 (Opening).

Hi Sorin,

If you want to calculate the radiographic sensitivity when using the wire IQI, you can use this formula .
Thickness of the thinnest wire x 100%
Sensitivity = -------------------------------------------------
Material thickness
AS you know you need 2% sensitivity for accept to radiography film. I have DIN & ISO IQI sensitivity chart that is alrady calculated . If you wants contact me.
Regard

 
 Reply 
 
John carpenter
John carpenter
01:29 Aug-13-2013
Re: Wire IQI
In Reply to shahid at 13:49 Aug-12-2013 .

Thank you very much guys for the info.
Shahid if can give me those charts I would realy appreciate it.

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 877

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
877
02:10 Aug-13-2013
Re: Wire IQI
In Reply to John carpenter at 01:29 Aug-13-2013 .

John,

Have a look at ASTM E747. In there it gives you the equivalence for hole and wire type penetrameters.

 
 Reply 
 
EDUARDO VERZOSA
EDUARDO VERZOSA
08:36 Dec-23-2013
Re: Wire IQI
In Reply to shahid at 13:49 Aug-12-2013 .


kindly gave to me the information ASTM of 4A & 4B WIRE DIAMETER CHART


 
 Reply 
 

Product Spotlight

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window