21:08 Aug-11-2013
Wire IQI

Hello everyoane,
How you calculate the radiographic sensitivity when using the wire IQI.I only used the hole type penetrameters, but now there s a European customer that want us to use the wire type.I know there are some standards out there, but maybe somebody can explain it to me much clearer.Thank you

 
 Reply 
 
andrew cunningham
NDT Inspector
Canada, Joined Jun 2008, 238

andrew cunningham

NDT Inspector
Canada,
Joined Jun 2008
238
23:30 Aug-11-2013
Re: Wire IQI
In Reply to John carpenter at 21:08 Aug-11-2013 (Opening).

If you are shooting through 100mm of steel and you can see a IQI 1mm wire. I would think you would have 1% But I could be wrong.

 
 Reply 
 
John carpenter
John carpenter
23:42 Aug-11-2013
Re: Wire IQI
In Reply to andrew cunningham at 23:30 Aug-11-2013 .

Thank you for your answer, but I think there s a formula that need to be applied based on the thinnest wire visible.Anyway if somebody have experience working with this type of IQI please give me some feedback.

 
 Reply 
 
Ed T.
Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III, Saudi Arabia, Joined Sep 2011, 169

Ed T.

Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III,
Saudi Arabia,
Joined Sep 2011
169
08:12 Aug-12-2013
Re: Wire IQI
In Reply to John carpenter at 23:42 Aug-11-2013 .

I believe this is correct.

Calculate the radiographic sensitivity for a wire-type penetrameter using the formula:

Sensitivity (%) = Thickness of the thinnest wire * 100/Specimen thickness

 
 Reply 
 
shahid
NDT Inspector,
Pakistan, Joined Mar 2013, 10

shahid

NDT Inspector,
Pakistan,
Joined Mar 2013
10
13:49 Aug-12-2013
Re: Wire IQI
In Reply to John carpenter at 21:08 Aug-11-2013 (Opening).

Hi Sorin,

If you want to calculate the radiographic sensitivity when using the wire IQI, you can use this formula .
Thickness of the thinnest wire x 100%
Sensitivity = -------------------------------------------------
Material thickness
AS you know you need 2% sensitivity for accept to radiography film. I have DIN & ISO IQI sensitivity chart that is alrady calculated . If you wants contact me.
Regard

 
 Reply 
 
John carpenter
John carpenter
01:29 Aug-13-2013
Re: Wire IQI
In Reply to shahid at 13:49 Aug-12-2013 .

Thank you very much guys for the info.
Shahid if can give me those charts I would realy appreciate it.

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 877

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
877
02:10 Aug-13-2013
Re: Wire IQI
In Reply to John carpenter at 01:29 Aug-13-2013 .

John,

Have a look at ASTM E747. In there it gives you the equivalence for hole and wire type penetrameters.

 
 Reply 
 
EDUARDO VERZOSA
EDUARDO VERZOSA
08:36 Dec-23-2013
Re: Wire IQI
In Reply to shahid at 13:49 Aug-12-2013 .


kindly gave to me the information ASTM of 4A & 4B WIRE DIAMETER CHART


 
 Reply 
 

Product Spotlight

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window