Taking thickness readings on FRP material.

I would like to find out if there is such a thing as a, UT transducer, that is able to take thickness readings of FRP pipe material. (* FRP = Fiber Reinforced Plastic *)

I don't think that a transducer would be able to use sound to obtain a thickness reading due to the amout of glass fiber in the material. But then again, I could be completely wrong and need to be shown the light.

Thanks,
K Fosha


 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 159

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
159
06:28 Dec-18-2002
Re: Taking thickness readings on FRP material.
: I would like to find out if there is such a thing as a, UT transducer, that is able to take thickness readings of FRP pipe material. (* FRP = Fiber Reinforced Plastic *)
.
: I don't think that a transducer would be able to use sound to obtain a thickness reading due to the amout of glass fiber in the material. But then again, I could be completely wrong and need to be shown the light.
.
: Thanks,
: K Fosha
.
Over the years I have had a number of experiences with FRP. Krautkramer once had a thickness gauge the CL202F which uses the ZIP zero interface probe, it is now no longer available. This probe works well as it is a 0.5MHz probe with a special delay block to reduce the interface echo, ( as the name implies). Details can be found on the KK website about ZIP probes.

Recently we have been using the piezo-composite probes for testing FRP pipe and rubber conveyor belt with great success. Try the K1SC, MSEK2 and MK1S

Regards

Neil Burleigh


 
 Reply 
 
Taha R Sheikh
Taha R Sheikh
18:01 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to Neil Burleigh at 06:28 Dec-18-2002 .

hello neil,

i just read ur reply below.

unfortuatly i cant get any of the below mentioned products in KK website.
Please send me the link or advice me accordingly for thickness montioring of FRP ducts!

taha

 
 Reply 
 
Sudheer Jai Krishnan
Sudheer Jai Krishnan
21:01 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to Taha R Sheikh at 18:01 Feb-28-2013 .

Hello Taha

Please let us know your min and maximum thickness. Have you tried a 45MG or a 38DL Plus for the thickness measurements? If not please see the link below and We have given solutions for similar kind of application to many of our customers. The highlighting feature is that ,the 38DLP has got both precision thickness measurements and corrosion measurements such that you can have one equipment for your different requirements

Kindly let me know if i can be of any assistance to you.

http://www.olympus-ims.com/en/38dl-plus/

Regards

Sudheer Jai Krishnan

 
 Reply 
 
James Scalf
NDT Inspector,
Global Integrity, Canada, Joined Oct 2012, 274

James Scalf

NDT Inspector,
Global Integrity,
Canada,
Joined Oct 2012
274
21:04 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to Sudheer Jai Krishnan at 21:01 Feb-28-2013 .

Taha,

Another option is the new Zip line of probes available through General Electric... Check online to find a representative near you...

 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
21:06 Feb-28-2013
Re: Taking thickness readings on FRP material.
In Reply to K Fosha at 02:14 Dec-17-2002 (Opening).

Yes, there are transducers suitable for fiberglass testing. For more than 25 years Panametrics and now Olympus NDT has offered a specialized 500 KHz delay line transducer, the M2008, that is optimized for thickness measurement and detection of laminar flaws in fiberglass up to 100 mm or thicker. It uses an impedance matched delay line for good coupling and minimal interface echo interference. It can be used with high penetration thickness gages or with a flaw detector. The application note in the link below references fiberglass boat hulls, but the principle is applicable to fiberglass pipes as well.

http://www.olympus-ims.com/en/applications/thickness-gaging-fiberglass-boat-hulls/

We (and other major manufacturers as well) also offer a number of other low frequency transducers that can be effectively used on fiberglass in various thickness ranges. If your pipe radius is less than approximately 150 mm we would first try a smaller diameter transducer as an alternative, such as a 1 MHz or 2.25 MHz, 12.5 mm diameter broadband contact transducer.

 
 Reply 
 

Product Spotlight

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window