Technical Discussions
hemant suthar
hemant suthar
09:21 Mar-03-2010
regarding asme sec-ix group no.

what is the purpose of group no. in asme sec-ix and on what base it classified.

 
 Reply 
 
Roger Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
18:05 Mar-04-2010
Re: regarding asme sec-ix group no.
In Reply to hemant suthar at 09:21 Mar-03-2010 (Opening).

Mr. Suthar, if you mean Group# [versus P#], the Group#'s are subsets of the P#'s that group materials with similar heat-input and heat-treatment characteristics, per ASME Section IX.
Group# is a Supplementary Essential Variable, and is used for controlled heat input Weld Procedures, like when the Impact Strength at Low Temperature is being tested and recorded during the Procedure Qualification.

 
 Reply 
 
Ganesh V
Other, Site Inspection Supervisor
PDO,Oman, India, Joined Jun 2013, 5

Ganesh V

Other, Site Inspection Supervisor
PDO,Oman,
India,
Joined Jun 2013
5
07:19 Jun-07-2013
Re: regarding asme sec-ix group no.
In Reply to hemant suthar at 09:21 Mar-03-2010 (Opening).

Group Numbers are assigned additionally to P-Numbers. These Group Numbers classify the metals within P-Numbers for the purpose of procedure qualification where notch-toughness ( Charpy V-notch impact test ) requirements are specified.
( Refer : QW.200.3 )

So, whenever the codes requires Impact testing, WPS shall specify the Supplimentary essential variables also, and PQR shall reflect the actual p Number's and its applicable Group Numbers, any changes after in WPS need to be requalified with a PQR again.

 
 Reply 
 
Nelson
Nelson
14:21 Sep-18-2013
Re: regarding asme sec-ix group no.
In Reply to Roger Duwe at 18:05 Mar-04-2010 .

Dear Roger Duwe,

Good info you give. How can i refer that it is related with "similar heat input & heat treatment characteristics" in code. i.e, any asme state these group number has been classified according to this? Please reply.
Thanks in advance.

Neo.

 
 Reply 
 
Roger D. Duwe
NDT Inspector, API-510, 570, 653
MISTRAS, USA, Joined Jan 2009, 148

Roger D. Duwe

NDT Inspector, API-510, 570, 653
MISTRAS,
USA,
Joined Jan 2009
148
19:38 Sep-18-2013
Re: regarding asme sec-ix group no.
In Reply to Nelson at 14:21 Sep-18-2013 .

Nelson, that is so basic that the answer is almost hard. This info comes from the definition of "P#" and "Group#". It is part of the foundation of ASME Sect IX. Without it, every different material spec & grade would require its own individualized PQR and WPS.

 
 Reply 
 

Product Spotlight

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

On-Demand Webinar: Advanced Ultrasonic Techniques for HTHA Detection & Assessment

In the Oil and Gas industry, High Temperature Hydrogen Attack (HTHA) can occur in steels operating a
...
t high temperature, usually above 205°C (400°F). Early stages of HTHA are very difficult to detect. Join us for a webinar presented by Guy Maes, Zetec Sales Engineer Director. The webinar will demonstrate how advanced ultrasonic techniques are deployed for efficient and reliable HTHA inspections.
>