19:47 Sep-10-2013
ASME MT Examination Procedure

Can someone help me out here.
ASME V Article 7 states "Equipment of the same type" as a Nonessential Variable.
What is this referring to?
Thanks
Stan

 
 Reply 
 
Ed T.
Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III, Saudi Arabia, Joined Sep 2011, 169

Ed T.

Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III,
Saudi Arabia,
Joined Sep 2011
169
07:11 Sep-17-2013
Re: ASME MT Examination Procedure
In Reply to member at 19:47 Sep-10-2013 (Opening).

Just a guess, but I would think that they are referring to types of equipment as yokes, pirtable MT units, etc.
To me, the brand of yoke used would not be an essential variable.

 
 Reply 
 
Derek
Derek
02:19 Sep-26-2013
Re: ASME MT Examination Procedure
In Reply to Ed T. at 07:11 Sep-17-2013 .

The intent is that you can perform circular magnetization using a horizontal bench or portable unit, while longitudinal magnetization may be completed using a yoke or other means determined by the procedure. This can be a necessary technique since some part configurations or sizes make the use of a coil or cable wrap impractical or do not allow it. Per ASME Section V Article 7: If the L/D Ratio is Less than 2 you shall not use a coil for longitudinal magnetization. This would require you the use an alternate method to perform the required inspection in accordance with this code such as a yoke.

 
 Reply 
 

Product Spotlight

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window