cracks inside Al/CFRP assembly

Could anyone suggest me a way to control an assembly of Al(17mm)+CFRP(18mm)+Al(45mm)+CFRP(33mm)+Al(37mm)in what regards cracks at the third layer?
And with what accuracy?
Thanks in advance.


 
 Reply 
 
Jens Forker
Jens Forker
07:57 Jan-21-2003
Re: cracks inside Al/CFRP assembly
Hi,
AE may be of help here, but I would need more details (actual scope of testing, size/geometry of your component/part,...) to estimate if AE would really do the expected job.
Please send the details + your address to my email that I can provide further information.
regards
Jens

: Could anyone suggest me a way to control an assembly of Al(17mm)+CFRP(18mm)+Al(45mm)+CFRP(33mm)+Al(37mm)in what regards cracks at the third layer?
: And with what accuracy?
: Thanks in advance.
.



 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window