some questions regarding impact echo

I have some questions regarding NDE and impact echo in particular, for concrete pipes.
1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
3)why are S-waves ignored in impact echo testing?

Thanx advance for your answers




 
 Reply 
 
kavita
kavita
00:01 Jan-25-2003
one more question
: I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: 3)why are S-waves ignored in impact echo testing?
. 4)what is the difference between impact-echo and impulse response. is it that in impulse response the stress wave is generated by a transmitter and in impact-echo that is done by mechanical impact.
: Thanx advance for your answers
.



 
 Reply 
 
Franc Buijsen
Franc Buijsen
03:09 Jan-25-2003
Re: some questions regarding impact echo
I advise you to contact a company called Andec in Toronto Canada, andec@andec.on.ca. They are very familiar with concrete testing using impact echo.

regards

Franc

: I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: 3)why are S-waves ignored in impact echo testing?
.
: Thanx advance for your answers
.



 
 Reply 
 
Christian Grosse
Teacher,
Technische Universität München, Germany, Joined Nov 2000, 11

Christian Grosse

Teacher,
Technische Universität München,
Germany,
Joined Nov 2000
11
02:42 Jan-31-2003
Re: some questions regarding impact echo
These are several interesting questions and a discussion could be
useful. I am not an expert in SASW, but maybe you can point to a proper
source of information.

Regarding question 3 I am not sure if I understand the benefit you
expect to get using S-waves additionally to P-waves. However, since the
impact usually used in impact-echo testing produces mainly compressional
waves, I would not expect S-waves to be very dominant. These problems
are now addressed by a collaborative research project in Germany (see
http://www.for384.uni-stuttgart.de/) using a combination of experiments
and simulations. The answer is: This is ongoing research.

If you understand impulse response as a technique generating stress
waves by ultrasound emitters, this could be a difference to impact-echo.
To generate high amplitude pulses usually piezo-electric emitters of the
resonant type are used. The idea of impact-echo is instead to use
broadband pulses (pulses with energy over a broader frequency band) to
detect "reverbations" caused by flaws in different depth. This is
another difference to most ultrasound impulse techniques. The amplitudes
generated by broadband piezo-electric emitters are usually too weak.

Christian Grosse


---------------------------------
: I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: 3)why are S-waves ignored in impact echo testing?
.
: Thanx advance for your answers
.



 
 Reply 
 
kavita
kavita
00:33 Feb-05-2003
Re: some questions regarding impact echo
Thank You Mr.Grosse!


 
 Reply 
 
WILLIAM A. WEBER
Director
IMPACT-ECHO INSTRUMENTS,LLC, USA, Joined Mar 2003, 2

WILLIAM A. WEBER

Director
IMPACT-ECHO INSTRUMENTS,LLC,
USA,
Joined Mar 2003
2
06:16 Mar-24-2003
Re: some questions regarding impact echo
: These are several interesting questions and a discussion could be
: useful. I am not an expert in SASW, but maybe you can point to a proper
: source of information.
.
: Regarding question 3 I am not sure if I understand the benefit you
: expect to get using S-waves additionally to P-waves. However, since the
: impact usually used in impact-echo testing produces mainly compressional
: waves, I would not expect S-waves to be very dominant. These problems
: are now addressed by a collaborative research project in Germany (see
: http://www.for384.uni-stuttgart.de/) using a combination of experiments
: and simulations. The answer is: This is ongoing research.
.
: If you understand impulse response as a technique generating stress
: waves by ultrasound emitters, this could be a difference to impact-echo.
: To generate high amplitude pulses usually piezo-electric emitters of the
: resonant type are used. The idea of impact-echo is instead to use
: broadband pulses (pulses with energy over a broader frequency band) to
: detect "reverbations" caused by flaws in different depth. This is
: another difference to most ultrasound impulse techniques. The amplitudes
: generated by broadband piezo-electric emitters are usually too weak.
.
: Christian Grosse
.
:
: ---------------------------------
: : I have some questions regarding NDE and impact echo in particular, for concrete pipes.
: : 1)Has ever been SASW (spectral analysis of surface waves) been used for evaluating the integrity of concrete pipe. Can anybody give me a case study?
: : 2)I've read some where that SASW and impact echo are similar to some extent. to what extent are they similar and hpw are they different.
: : 3)why are S-waves ignored in impact echo testing?
: .
: : Thanx advance for your answers
: .
.CHRISTIAN,

TAKE A LOOK AT OUR WEBSITE, WWW.IMPACT-ECHO.COM; IT HAS CASE HISTORIES AND LOTS OF INFO. WE ALSO SELL THE BOOK ON THE TOPIC WHICH WILL ANSWER ALL YOUR QUESTIONS. SORRY NOT TO REPLY SOONER, BUT I JUST SAW YOUR QUESTION.

BILL WEBER



 
 Reply 
 

Product Spotlight

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window