Jose Rios
Jose Rios
07:50 Nov-10-1998
bimorph bender transducer

Dear experts,

to develop a present application I would need design a bimorph bender tranduscer in parallel configuration. I believe that the response of such a transducer depends only on the dimensions (thickness, free length, clamped length, and width) of the bimorph as well as the piezoceramic material that compounds.

My question is how, or in other words what is the relation between the response of the bimorph (bending in cantilever configuration) (resonance frequency, bandwidth, displacement, voltage needed...) and its dimensions (T, FL, CL, W) and nature. How should be designed, starting from the response specifications, the dimensions and nature of the bender???

I would grateful any clues or references of books or web pages, journal articles... where it could be explained.

Thanks in advance.





 
 Reply 
 
Afshin Madinei
Afshin Madinei
09:13 Dec-23-1998
Re: bimorph bender transducer
: Dear experts,

: to develop a present application I would need design a bimorph bender tranduscer in parallel configuration. I believe that the response of such a transducer depends only on the dimensions (thickness, free length, clamped length, and width) of the bimorph as well as the piezoceramic material that compounds.

: My question is how, or in other words what is the relation between the response of the bimorph (bending in cantilever configuration) (resonance frequency, bandwidth, displacement, voltage needed...) and its dimensions (T, FL, CL, W) and nature. How should be designed, starting from the response specifications, the dimensions and nature of the bender???

: I would grateful any clues or references of books or web pages, journal articles... where it could be explained.

: Thanks in advance.





 
 Reply 
 
M. Simon
M. Simon
01:12 Feb-19-1999
Re: bimorph bender transducer



 
 Reply 
 
Rainer Meier
R & D
retired from intelligeNDT Systems & Services, Germany, Joined Nov 1998, 15

Rainer Meier

R & D
retired from intelligeNDT Systems & Services,
Germany,
Joined Nov 1998
15
01:05 Feb-26-1999
Re: bimorph bender transducer
: Dear experts,

: to develop a present application I would need design a bimorph bender tranduscer in parallel configuration. I believe that the response of such a transducer depends only on the dimensions (thickness, free length, clamped length, and width) of the bimorph as well as the piezoceramic material that compounds.

: My question is how, or in other words what is the relation between the response of the bimorph (bending in cantilever configuration) (resonance frequency, bandwidth, displacement, voltage needed...) and its dimensions (T, FL, CL, W) and nature. How should be designed, starting from the response specifications, the dimensions and nature of the bender???

: I would grateful any clues or references of books or web pages, journal articles... where it could be explained.

: Thanks in advance.


The properties of bender widely vary depending on the design (monomorph, bimorph, trimorph), driving
conditions and PZT material. Basic relations for example are given in the company paper
"Piecoelectric Ceramics", Philips Components, Eindhoven, The Netherlands (1991). A paper covering
the topic with 95 citations: Jan G. Smits et al., Sensors and Actuators A, 28 (1991) pp. 41 - 61.

Rainer Meier
on behalf of
Dr. Karl Lubitz
E-mail: Karl.Lubitz@mchp.siemens.de



 
 Reply 
 
k.rochdi
k.rochdi
03:08 Mar-16-1999
Re: bimorph bender transducer
: : Dear experts,

: : to develop a present application I would need design a bimorph bender tranduscer in parallel configuration. I believe that the response of such a transducer depends only on the dimensions (thickness, free length, clamped length, and width) of the bimorph as well as the piezoceramic material that compounds.

: : My question is how, or in other words what is the relation between the response of the bimorph (bending in cantilever configuration) (resonance frequency, bandwidth, displacement, voltage needed...) and its dimensions (T, FL, CL, W) and nature. How should be designed, starting from the response specifications, the dimensions and nature of the bender???

: : I would grateful any clues or references of books or web pages, journal articles... where it could be explained.

: : Thanks in advance.

:
: The properties of bender widely vary depending on the design (monomorph, bimorph, trimorph), driving
: conditions and PZT material. Basic relations for example are given in the company paper
: "Piecoelectric Ceramics", Philips Components, Eindhoven, The Netherlands (1991). A paper covering
: the topic with 95 citations: Jan G. Smits et al., Sensors and Actuators A, 28 (1991) pp. 41 - 61.

: Rainer Meier
: on behalf of
: Dr. Karl Lubitz
: E-mail: Karl.Lubitz@mchp.siemens.de




 
 Reply 
 

Product Spotlight

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window