Hello everyoane,
How you calculate the radiographic sensitivity when using the wire IQI.I only used the hole type penetrameters, but now there s a European customer that want us to use the wire type.I know there are some standards out there, but maybe somebody can explain it to me much clearer.Thank you

 
 Reply 
 
andrew cunningham
NDT Inspector
Canada, Joined Jun 2008, 238

andrew cunningham

NDT Inspector
Canada,
Joined Jun 2008
238
23:30 Aug-11-2013
Re: Wire IQI
In Reply to John carpenter at 21:08 Aug-11-2013 (Opening).

If you are shooting through 100mm of steel and you can see a IQI 1mm wire. I would think you would have 1% But I could be wrong.

 
 Reply 
 
John carpenter
John carpenter
23:42 Aug-11-2013
Re: Wire IQI
In Reply to andrew cunningham at 23:30 Aug-11-2013 .

Thank you for your answer, but I think there s a formula that need to be applied based on the thinnest wire visible.Anyway if somebody have experience working with this type of IQI please give me some feedback.

 
 Reply 
 
Ed T.
Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III, Saudi Arabia, Joined Sep 2011, 169

Ed T.

Other, ASNT Level III, UT, RT, MT, PT, VT
NDT Level III,
Saudi Arabia,
Joined Sep 2011
169
08:12 Aug-12-2013
Re: Wire IQI
In Reply to John carpenter at 23:42 Aug-11-2013 .

I believe this is correct.

Calculate the radiographic sensitivity for a wire-type penetrameter using the formula:

Sensitivity (%) = Thickness of the thinnest wire * 100/Specimen thickness

 
 Reply 
 
shahid
NDT Inspector,
Pakistan, Joined Mar 2013, 10

shahid

NDT Inspector,
Pakistan,
Joined Mar 2013
10
13:49 Aug-12-2013
Re: Wire IQI
In Reply to John carpenter at 21:08 Aug-11-2013 (Opening).

Hi Sorin,

If you want to calculate the radiographic sensitivity when using the wire IQI, you can use this formula .
Thickness of the thinnest wire x 100%
Sensitivity = -------------------------------------------------
Material thickness
AS you know you need 2% sensitivity for accept to radiography film. I have DIN & ISO IQI sensitivity chart that is alrady calculated . If you wants contact me.
Regard

 
 Reply 
 
John carpenter
John carpenter
01:29 Aug-13-2013
Re: Wire IQI
In Reply to shahid at 13:49 Aug-12-2013 .

Thank you very much guys for the info.
Shahid if can give me those charts I would realy appreciate it.

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 889

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
889
02:10 Aug-13-2013
Re: Wire IQI
In Reply to John carpenter at 01:29 Aug-13-2013 .

John,

Have a look at ASTM E747. In there it gives you the equivalence for hole and wire type penetrameters.

 
 Reply 
 
EDUARDO VERZOSA
EDUARDO VERZOSA
08:36 Dec-23-2013
Re: Wire IQI
In Reply to shahid at 13:49 Aug-12-2013 .


kindly gave to me the information ASTM of 4A & 4B WIRE DIAMETER CHART


 
 Reply 
 

Product Spotlight

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window