Defects manufacturer wanted - Can you make defects ?

Hi,
we are looking for European companies that have expertise in manufacturing defects and more especially SCC types (but also more conventional types).
If you know of companies that could help us please let us know their name and possible URL.
Thank you.
PL


 
 Reply 
 
John hansen
Director, - Eddy Current Technology
ETher NDE Ltd, United Kingdom, Joined Oct 1999, 74

John hansen

Director, - Eddy Current Technology
ETher NDE Ltd,
United Kingdom,
Joined Oct 1999
74
04:17 Feb-28-2003
Re: Defects manufacturer wanted - Can you make defects ?
Try TrueFlaw from Finland I think.

www.trueflaw.com

Rgds

John Hansen
www.hocking.com



 
 Reply 
 
Joe Buckley, Sonatest PLc
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley, Sonatest PLc

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
04:28 Feb-28-2003
Re: Defects manufacturer wanted - Can you make defects ?
In the UK, Sonaspection have pretty good capabilities
-Depends exactly what you need

http://www.sonaspection.co.uk

Good Luck
Joe


: Hi,
: we are looking for European companies that have expertise in manufacturing defects and more especially SCC types (but also more conventional types).
: If you know of companies that could help us please let us know their name and possible URL.
: Thank you.
: PL
.



 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
04:44 Feb-28-2003
Re: Defects manufacturer wanted - Can you make defects ?
PL,

My company makes IGSCC/SCC type cracks in SS materials. We have a procedure for Carbon Steel too.

For regular flaws contact Sonaspcection.

J. Mark Davis
Davis NDE, Inc.
(205) 663-7006


Hi,
: we are looking for European companies that have expertise in manufacturing defects and more especially SCC types (but also more conventional types).
: If you know of companies that could help us please let us know their name and possible URL.
: Thank you.
: PL
.




 
 Reply 
 
Phil Herman Jr.
Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards, USA, Joined Oct 1999, 79

Phil Herman Jr.

Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards,
USA,
Joined Oct 1999
79
05:39 Feb-28-2003
Re: Defects manufacturer wanted - Can you make defects ?
In addition to the two companies mentioned previously, you may try contacting FlawTech Inc. at www.flawtech.com.

Good Luck with your search.
Phil Herman Jr.
PH Tool Reference Standards

: Hi,
: we are looking for European companies that have expertise in manufacturing defects and more especially SCC types (but also more conventional types).
: If you know of companies that could help us please let us know their name and possible URL.
: Thank you.
: PL
.



 
 Reply 
 
Niklas Larsson
Niklas Larsson
08:31 Mar-03-2003
Re: Defects manufacturer wanted - Can you make defects ?
Uddcomb Engineering in Sweden is also an company that maybe can help you.
http://www.uddcomb.se/Pages/EngelskaPages/engelskaframestes/engframesetkraft.html

Regards
Niklas Larsson
SQC


: Hi,
: we are looking for European companies that have expertise in manufacturing defects and more especially SCC types (but also more conventional types).
: If you know of companies that could help us please let us know their name and possible URL.
: Thank you.
: PL
.



 
 Reply 
 
Niklas Larsson
Niklas Larsson
08:31 Mar-03-2003
Re: Defects manufacturer wanted - Can you make defects ?
Uddcomb Engineering in Sweden is also an company that maybe can help you.
http://www.uddcomb.se/Pages/EngelskaPages/engelskaframestes/engframesetkraft.html

Regards
Niklas Larsson
SQC


: Hi,
: we are looking for European companies that have expertise in manufacturing defects and more especially SCC types (but also more conventional types).
: If you know of companies that could help us please let us know their name and possible URL.
: Thank you.
: PL
.



 
 Reply 
 

Product Spotlight

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window