about fiberglass construction

Hi, everyone.
Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
N. Azarov


 
 Reply 
 
ISOTEST Engineering S.r.l.
Director
ISOTEST ENGINEERING SRL, Italy, Joined May 2002, 2

ISOTEST Engineering S.r.l.

Director
ISOTEST ENGINEERING SRL,
Italy,
Joined May 2002
2
09:10 Mar-04-2003
re: About fiberglass construction
: Hi, everyone.
: Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
: N. Azarov
.
We have obtained very good results in the control of this materials with air coupled Ultrasounds.
If you want to know more about this "new" methods, please ask.

Bye


 
 Reply 
 
Richard Kazares
Richard Kazares
03:46 Mar-04-2003
Re: re: About fiberglass construction
You might also look at squirter/bubbler (mechanical contour following) techniques using relatively low-cost water-based (recirculation - low volume of water) conventional UT. The advantagesl are that much higher frequencies can be used - resulting in higher resolution images - that are both easier to interpret - as well as providing more detailed information.

Contact me directly - and I'll be happy to e-mail you some honeycomb images taken using this technology and system configuration.

: : Hi, everyone.
: : Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
: : N. Azarov
: .


 
 Reply 
 

Product Spotlight

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>