Renaningsih Setjo
Renaningsih Setjo
08:30 Mar-04-2003
Material designation

Dear Colleagues,

At present I have been working in Material Testing Lab. I am doing research on Remaining Life for boiler tubes. The material of the tubes are 15 No.3, 10 Cr No.910, ST 35.8 III.
I have the difficulties to get some data related to the chemical composituion of these materials since I am not familiar with this designation. Dear Friend would you please help me with the equal design. of these materials according to ASTM Code?? ...Please inform..I really appreciated for your help.


Best regards

Ms. Rena Setjo


 
 Reply 
 
Uli Mletzko
R & D, Retired
Germany, Joined Nov 1998, 89

Uli Mletzko

R & D, Retired
Germany,
Joined Nov 1998
89
00:23 Mar-04-2003
Re: Material designation

: At present I have been working in Material Testing Lab. I am doing research on Remaining Life for boiler tubes. The material of the tubes are 15 No.3, 10 Cr No.910, ST 35.8 III.
: I have the difficulties to get some data related to the chemical composituion of these materials since I am not familiar with this designation. Dear Friend would you please help me with the equal design. of these materials according to ASTM Code?? ...Please inform..I really appreciated for your help.

Dear Ms. Rena Setjo,
the materials mentioned are according to German standards (DIN), for low or medium temperature boiler applications.

The composition is for

St_35.8 = (C <= 0.17 %, Si <= 0.35 %, Mn >= 0.40 %, Cr <= 0.03 %),
15_Mo_3 = (C 0.12-0.20 %, Si 0.15-0.35 %, Mn 0.50-0.80 %, Cr <= 0.03 %, Mo 0.25-0.35 %),
10_CrMo_9_10 = (C <= 0.15 %, Si 0.15-0.50 %, Mn 0.40-0.60 %, Cr 2.0-2.5 %, Mo 0.9-1.1 %).

The roman number 'III' is for quality level 'three'.

I've used the underscore character '_' within the alloy names. In the original names there have to be blanks/spaces.

The ranking is ascending according to the alloy content of molybdenum and chromium, which is according to the intended temperature level.

I hope this helps to find corresponding alloys according to other standards.

Regards
Uli Mletzko
MPA, NDT group,
University of Stuttgart, Germany



 
 Reply 
 

Product Spotlight

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window