N. Azarov
Engineering
GosNIIGA, Russia, Joined Jan 2000, 12

N. Azarov

Engineering
GosNIIGA,
Russia,
Joined Jan 2000
12
09:49 Mar-01-2003
about fiberglass construction

Hi, everyone.
Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
N. Azarov


 
 Reply 
 
ISOTEST Engineering S.r.l.
Director
ISOTEST ENGINEERING SRL, Italy, Joined May 2002, 2

ISOTEST Engineering S.r.l.

Director
ISOTEST ENGINEERING SRL,
Italy,
Joined May 2002
2
09:10 Mar-04-2003
re: About fiberglass construction
: Hi, everyone.
: Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
: N. Azarov
.
We have obtained very good results in the control of this materials with air coupled Ultrasounds.
If you want to know more about this "new" methods, please ask.

Bye


 
 Reply 
 
Richard Kazares
Richard Kazares
03:46 Mar-04-2003
Re: re: About fiberglass construction
You might also look at squirter/bubbler (mechanical contour following) techniques using relatively low-cost water-based (recirculation - low volume of water) conventional UT. The advantagesl are that much higher frequencies can be used - resulting in higher resolution images - that are both easier to interpret - as well as providing more detailed information.

Contact me directly - and I'll be happy to e-mail you some honeycomb images taken using this technology and system configuration.

: : Hi, everyone.
: : Does anybody know, where can find the information about methods of non-destructive testing of quality adhesion skins from fiberglass in honeycomb constructions of a rudder, elevators, flaps of airplanes.
: : N. Azarov
: .


 
 Reply 
 

Product Spotlight

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>