where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
480 views
Technical Discussions
Renaningsih Setjo
Renaningsih Setjo
08:30 Mar-04-2003
Material designation

Dear Colleagues,

At present I have been working in Material Testing Lab. I am doing research on Remaining Life for boiler tubes. The material of the tubes are 15 No.3, 10 Cr No.910, ST 35.8 III.
I have the difficulties to get some data related to the chemical composituion of these materials since I am not familiar with this designation. Dear Friend would you please help me with the equal design. of these materials according to ASTM Code?? ...Please inform..I really appreciated for your help.


Best regards

Ms. Rena Setjo


 
 Reply 
 
Uli Mletzko
R & D, Retired
Germany, Joined Nov 1998, 89

Uli Mletzko

R & D, Retired
Germany,
Joined Nov 1998
89
00:23 Mar-04-2003
Re: Material designation

: At present I have been working in Material Testing Lab. I am doing research on Remaining Life for boiler tubes. The material of the tubes are 15 No.3, 10 Cr No.910, ST 35.8 III.
: I have the difficulties to get some data related to the chemical composituion of these materials since I am not familiar with this designation. Dear Friend would you please help me with the equal design. of these materials according to ASTM Code?? ...Please inform..I really appreciated for your help.

Dear Ms. Rena Setjo,
the materials mentioned are according to German standards (DIN), for low or medium temperature boiler applications.

The composition is for

St_35.8 = (C <= 0.17 %, Si <= 0.35 %, Mn >= 0.40 %, Cr <= 0.03 %),
15_Mo_3 = (C 0.12-0.20 %, Si 0.15-0.35 %, Mn 0.50-0.80 %, Cr <= 0.03 %, Mo 0.25-0.35 %),
10_CrMo_9_10 = (C <= 0.15 %, Si 0.15-0.50 %, Mn 0.40-0.60 %, Cr 2.0-2.5 %, Mo 0.9-1.1 %).

The roman number 'III' is for quality level 'three'.

I've used the underscore character '_' within the alloy names. In the original names there have to be blanks/spaces.

The ranking is ascending according to the alloy content of molybdenum and chromium, which is according to the intended temperature level.

I hope this helps to find corresponding alloys according to other standards.

Regards
Uli Mletzko
MPA, NDT group,
University of Stuttgart, Germany



 
 Reply 
 

Product Spotlight

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

MIZ®-21C: Truly Affordable Eddy Current Handheld with Surface Array Capability

Introducing MIZ-21C, the first truly affordable handheld eddy current instrument with surface array
...
capabilities. MIZ-21C can deliver fast, accurate inspections in demanding NDT applications including aerospace, oil and gas, manufacturing, and power generation. The surface array solution can reduce inspection time by up to 95% compared to traditional handheld pencil probes. The ergonomic design, long battery life, and intuitive touchscreen mean you can inspect more areas faster than ever without fatigue.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>