Sound velocity of Aluminium

I will soon be in the process of ultrasonically inspecting the thickness of the fuselage of several old Bonanza Aircraft. Could anybody please supply me with the velocity of sound for 2024 Aluminium?

Thank you


 
 Reply 
 
Jens Forker
Jens Forker
04:32 Mar-04-2003
Re: Sound velocity of Aluminium
Hi,
try the following:

www.Krautkramer.com/reference/reference1.htm
www.ultrasonic.com/tables/index.htm

regards
Jens Forker


: I will soon be in the process of ultrasonically inspecting the thickness of the fuselage of several old Bonanza Aircraft. Could anybody please supply me with the velocity of sound for 2024 Aluminium?
.
: Thank you
.



 
 Reply 
 
Roubini Marini
Roubini Marini
04:47 Mar-04-2003
Re: Sound velocity of Aluminium
>the velocity of sound for 2024 Aluminium?

Al-2024-T4 0.246 in/usec= 0.625 cm/usec
steel correction 1.060

R.MARINI
HELLENIC AEROSPACE INDUSTRY sa



 
 Reply 
 

Product Spotlight

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window