Velocity of stainless steel 316 and plexiglass

Please,

could anyone provide me with the ultrasound velocity of the following materials:
steel 316
plexiglass
perspex (lucite)

I really cannot find accurate values.

Thank you in advance.


 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 159

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
159
00:44 Mar-07-2003
Re: Velocity of stainless steel 316 and plexiglass
: Please,
.
: could anyone provide me with the ultrasound velocity of the following materials:
: steel 316
: plexiglass
: perspex (lucite)
.
: I really cannot find accurate values.
.
: Thank you in advance.
.Here is some info. for you
Lucite Vlong 2680m/sec Vshear 1050m/sec
Plexiglass a)UVA Vlong 2760m/sec Vshear 1090m/sec
b)UVAII Vlong 2730m/sec Vshear 1080m/sec
Hope this helps
Regards



 
 Reply 
 
Uli Mletzko
R & D, Retired
Germany, Joined Nov 1998, 89

Uli Mletzko

R & D, Retired
Germany,
Joined Nov 1998
89
04:24 Mar-07-2003
Re: Velocity of stainless steel 316 and plexiglass

: could anyone provide me with the ultrasound velocity of the following materials:
: steel 316

The ultrasound velocity in stainless steel is strongly depending on the material (cast, forged, weld), especially on the grain size and the grain orientation, leading to anisotropy.
In general, the velocity is lower than in heat treated, forged, fine grain ferritic carbon steel (clong = 5920 m/s, ctrans =3250 m/s).
So, clong = 5800 m/s might be a suitable average value, but sometimes it can be also down to 5400 m/s.
You have to use suitable control specimens or you have calibrate on the test specimen directly.

Regards
Uli Mletzko
NDT Group, MPA
University of Stuttgart, Germany


 
 Reply 
 
Kris Smestad
Kris Smestad
06:46 Mar-14-2003
Re: Velocity of stainless steel 316 and plexiglass
: Please,
.
: could anyone provide me with the ultrasound velocity of the following materials:
: steel 316
: plexiglass
: perspex (lucite)
.
: I really cannot find accurate values.
.
: Thank you in advance.

Keep it simple. If you have a known thickness of a material, you can determine it's exact velocity. Measure a sample with a micrometer. Set your screen range on your A-scan to twice that thickness. After compensating for probe delay, adjust your velocity so you have one signal at 50% and one at 100%.

Easy, right?
.



 
 Reply 
 

Product Spotlight

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window