where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

ZETEC, Inc.
Zetec is a global leader in nondestructive testing (NDT) solutions for the critical inspection needs of industries the world counts on every day, ...
4859 views
Technical Discussions
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
07:58 Jun-06-2007
ASME ultrasonic calibration blocks

The attached link is to an US company (Ray-Check) offering a set of alternative ASME calibration blocks manufactured in accordance with the Performance Demonstration Initiative (PDI), PDI-UT-1, Rev C (ferritic) and PD-UT-2, Rev C (austenitic).

A previous thread on ndt.net demonstrated the increased(unmanageable?) range of pipe calibration blocks required since the 2002 issue where Article 4 became Ultrasonic Examination of Welds:

http://www.ndt.net/wshop/forum/messages-1/9645.html

Ray-Check claim: "These cover the generic procedures for the ultrasonic examination of both ferritic and austenitic pipe welds. The blocks offer an economical alternative to fabricating multiple curved calibration blocks (pipe sections) in numerous diameters and wall thicknesses."

How can a set of 3 blocks (ferritic, 304 and 316 I believe) replace all those pipe nominal sizes and schedules supposedly required by T-434.3. I realise ASME is a pressure vessel rather than a piping code but unfortunately the piping codes (B31.3 and B31.4) specify use of ASME V and I can see no word in that document alowing use of these notched blocks. Even B31.3 Code Case 181 and ASME V Code Case 2235-9 require the manufacture of a qualification block of "the same product form, and material specification or equivalent P-Number grouping as one of the materials being examined. Has anyone experience with these "alternative blocks" iaw the PDI. Was this PDI run at EPRI? Why is there no mention of it in updates to ASME, how is anybody going ot learn about it apart from As our German colleagues say "reine Zufall".

I would be grateful for any enlightenment anybody can offer.





 
 Reply 
 
Aaron
Aaron
12:49 Feb-11-2014
Re: ASME ultrasonic calibration blocks
In Reply to Nigel Armstrong at 07:58 Jun-06-2007 (Opening).

I am hoping to revive this post and see if anyone out there has any insight on these blocks. I have not been able to find any ASME code cases that allow for the direct use of these. Also, where can you find the full PDI-UT-1, and -2? I have contacted a few of the manufacturers that are selling these blocks for more information and have not received any response back on. Any feedback would be appreciated. I also know that if I was to qualify these blocks individually on a job by job basis that they would be allowed, but I am trying to save time and money, so I am really looking for any documents that will allow the direct use of these alternative blocks. http://www.flawtech.com/proddetail.asp?prod=PDI-CB-4 Thanks everyone.

Aaron

 
 Reply 
 
Jason Witts
NDT Inspector,
Canada, Joined May 2011, 5

Jason Witts

NDT Inspector,
Canada,
Joined May 2011
5
19:49 Feb-11-2014
Re: ASME ultrasonic calibration blocks
In Reply to Aaron at 12:49 Feb-11-2014 .

The short answer would be no, these blocks would not be allowed according to code. For stainless steels not only should you have cal blocks of the same diameter/thickness of piece to be inspected.
You should also be demonstrating the system capabilities on a specimen welded according to the WPS used on the specific project.

 
 Reply 
 
John
John
03:32 Feb-12-2014
Re: ASME ultrasonic calibration blocks
In Reply to Jason Witts at 19:49 Feb-11-2014 .

Looked into those a few yrs back. Cannot use according to ASME the last time I checked. The word "SHALL" I believe applies in this situation.
Regards

 
 Reply 
 
Aaron
NDT Inspector,
USA, Joined Feb 2014, 1

Aaron

NDT Inspector,
USA,
Joined Feb 2014
1
13:07 Feb-12-2014
Re: ASME ultrasonic calibration blocks
In Reply to John at 03:32 Feb-12-2014 .

Thanks for the feedback. I thought these were too good to be true. However, I would love to see these PDI-UT-1 & 2 procedures to see what they are all about. What I don't understand is if the nuclear world (NRC and EPRI) have approved these through the performance demonstration initiative, why has ASME not made a code case about them. Nuclear inspections are to ASME section XI so if they are using these how are they not approved for regular ASME section V work of the same type (pipe butt welds). Also, if they are in use how is there not a code case about them? How are these companies getting away with selling these as an alternative to the standard ASME piping calibration blocks we all love so much. Has anyone seen these in use or know anyone that has used them? Still curious and hoping someone can provide more information on these. Thanks again.
Aaron

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1286

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1286
15:22 Feb-12-2014
Re: ASME ultrasonic calibration blocks
In Reply to John at 03:32 Feb-12-2014 .

Since Nigel posted this item in 2007 until now there has been a change in ASME Section V. In 2010 the paragraph T-434.3 Piping Calibration Blocks; describes how the basic calibration block configuration and reflectors shall be as shown in Fig. T-434.3.
But then departs from the old requirements to match schedule and allows curvature in accordance with T-434.1.7 and thickness ±25% of the nominal thickness of the component.
In a general way I echo John's statement about SHALL, however, ASME's statements concerning "shall" do not always mean mandatory. For example, T-434.4.1 states that the basic calibration blocks SHALL be as shown in Fig. T-434.4.1. Then in the very next paragraph T-434.4.2 provides for an alternative block. It is difficult to understand the term SHALL in the normal way that standards are written when it is accompanied by the concept of "or". This is seen in a few places in Section V. E.g. T-434.1.1 specified reflectors "SHALL" be used. Then in the next sentence they allow that an alternative be used.

1
 
 Reply 
 

Product Spotlight

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window